MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
AGC Asahiklin AE3000 Fluorinated Solvent
Categories: Fluid; Solvent

Material Notes: Asahiklin AE3000 is a fluorinated solvent used for cleaning, drying, and as a carrier solvent. This Hydrofluoroether (HFE-347pc-f) is a nonflammable solvent that has excellent material compatibility, low surface tension. Low Global Warming Potential, and Zero ODP.

Applications:

  • Precision cleaning of metals, alloys, composites, and plastics
  • Carrier solvent for fluorinated oils and greases
  • Carrier solvent for silicone oils
  • Drying agent after cleaning with hydrocarbons or alcohols
  • Particle removal
  • Replacement of HCFC, Dupornt™ Vertrel® & 3M™ Novec™ solvents
Benefits:
  • Non-flammable
  • Non-corrosive
  • Low global warming potential (GWP)
  • Zero ozone depletion potential (ODP)
  • Low surface tension, low viscosity, high liquid density
  • Excellent thermal, chemical, and hydrolytic stability
  • Superior drying property
  • Excellent permeability
  • Recyclable
  • Recoverable by simple distillation
  • Can be used with ultrasonics
  • No surfactants necessary

Information provided by AGC Chemicals Americas Inc.

Vendors:
Available Properties
  • Specific Gravity
  • Specific Gravity
  • Specific Gravity
  • Viscosity
  • Viscosity
  • Viscosity
  • Viscosity
  • Vapor Pressure
  • Vapor Pressure
  • Vapor Pressure
  • Surface Tension
  • Heat of Vaporization
  • Melting Point
  • Boiling Point
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Asahi Glass Company, AGC Fluorocompounds

Category Notes
none

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.