MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Hexcel® HexPly® M91 Epoxy Matrix
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: HexPly® M91 is a high performance, very tough epoxy matrix for use in aerospace primary structures and engines. HexPly® M91 is a toughened, controlled flow, epoxy resin system supplied with unidirectional fibers.

Benefits and Features

  • Excellent toughness with very high residual compression strength after impact.
  • Good translation of HexTow® fiber properties, both for intermediate modulus and high strength carbon fiber.
  • Designed for automation and particularly suited for both automated tape laying (ATL) and advanced fiber placement (AFP)
  • Good tack life and out-life, providing flexibility on the shop floor.
  • Low exotherm behavior allowing simple cures of thick monolithic structures up to 70mm (2.76”)
  • Dry Tg (DMA extrapolated onset E’) of 185°C-190°C (365°F-374°F)
  • Good hot-wet performance up to 120°C (250°F)

Information provided by Hexcel Corporation.

Vendors:
Available Properties
  • Viscosity, Monolithic Part < 15mm (0.6inch) thick
  • Viscosity, Monolithic Part 15mm-70mm (2.7inch) thick
  • Viscosity, Monolithic Part < 15mm (0.6inch) thick
  • Viscosity, Monolithic Part 15mm-70mm (2.7inch) thick
  • Viscosity, Monolithic Part < 15mm (0.6inch) thick
  • Viscosity, Monolithic Part 15mm-70mm (2.7inch) thick
  • Gel Time
  • Gel Time
  • Gel Time
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.