Notes: 430GHU BK400 is a 30% glass fiber reinforced Nylon 6 compound that contains 2% carbon black by weight for robust outdoor weathering performance Availability: Europe Fillers/Reinforcement: Glass Fiber, 30% Filler by Weight Additive: Carbon Black: 2%; Heat Stabilizer; UV Stabilizer Features: Heat Stabilized; Light Stabilized; Weather Resistant Form: Pellets Processing Method: Injection Molding Information provided by Teknor Apex |