Notes: ENF2 IS A 30% glass fiber reinforced, impact modified nylon 6 that offers good mechanical performance coupled with good surface finish. The grade also offers improved flow and is heat stabilized so that the good mechanical performance is maintained when exposed to elevated temperatures. The impact modification means that components in impact sensitive applications can be used without conditioning. Availability: Europe Fillers/Reinforcement: Glass Fiber, 30% Filler by Weight Additive: Heat Stabilizer; Impact Modifier Features: Good Surface Finish; Heat Stabilized; Impact Modified; Low Temperature Toughness Processing Method: Injection Molding Information provided by Teknor Apex |