MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Elmet Technologies
Solvay MTM® 71 Epoxy Matrix Resin
Categories: Polymer; Thermoset; Epoxy

Material Notes: Description: MTM71 prepreg is a toughened epoxy matrix resin pregreg system developed specifically for the manufacture of motorsport components, exhibiting excellent performance in the FIA side penetration test.

Features & Benefits:

  • 30 days out life at 21°C (70°F)
  • 12 months storage at -18°C(0°F)
  • Good tack and handling
  • Autoclave cure
  • 120°C (250°F) minimum cure
  • 155°C (310°F) Tg (DMA onset)
  • High levels of toughness for crash resistant motorsport structures
Note 1: Cure cycle: 1 hr at 135°C (275°F), 6.2 bar (90 psi)

CF4534 is a 283g/m2 5HS fabric with 12k T1000 type fibers; CF7234 is a 200g/m2 2x2 twill with 6k T1000 type fibers; CF2115 is a 200g/m2 2x2 twill fabric with 6k M46J fibers; CF1218 is a 200g/m2 2x2 twill fabric with 6k T800HB fibers

Information provided by Cytec, subsequently acquired by Solvay.

Vendors:
Available Properties
  • Density, Cured resin, 1 hr at 120°C + 2 hrs at 150°C
  • Storage Temperature, 12
  • Tensile Strength, ASTM D3039, 90°, M46J-124-36%, Note 1
  • Tensile Strength, ASTM D3039, 90°, T1000 GB-124-36%, Note 1
  • Tensile Strength, ASTM D3039, 90°, CF2115-42%, Note 1
  • Tensile Strength, ASTM D3039, 0°, CF2115-42%, Note 1
  • Tensile Strength, ASTM D3039, 90°, CF1218-42%, Note 1
  • Tensile Strength, ASTM D3039, 0°, CF1218-42%, Note 1
  • Tensile Strength, ASTM D3039, 90°, CF7234-42%, Note 1
  • Tensile Strength, ASTM D3039, 0°, CF7234-42%, Note 1
  • Tensile Strength, ASTM D3039, 90°, CF4534-42%, Note 1
  • Tensile Strength, ASTM D3039, 0°, CF4534-42%, Note 1
  • Tensile Strength, ASTM D3039, 0°, M46J-124-36%, Note 1
  • Tensile Strength, ASTM D3039, 0°, T1000 GB-124-36%, Note 1
  • Tensile Modulus, SACMA SRM01R94, 90°, M46J-124-36%, Note 1
  • Tensile Modulus, SACMA SRM01R94, 90°, T1000 GB-124-36%, Note 1
  • Tensile Modulus, SACMA SRM01R94, 90°, CF4534-42%, Note 1
  • Tensile Modulus, SACMA SRM01R94, 0°, CF1218-42%, Note 1
  • Tensile Modulus, SACMA SRM01R94, 0°, CF4534-42%, Note 1
  • Tensile Modulus, SACMA SRM01R94, 90°, CF1218-42%, Note 1
  • Tensile Modulus, SACMA SRM01R94, 0°, CF7234-42%, Note 1
  • Tensile Modulus, SACMA SRM01R94, 90°, CF7234-42%, Note 1
  • Tensile Modulus, SACMA SRM01R94, 90°, CF2115-42%, Note 1
  • Tensile Modulus, SACMA SRM01R94, 0°, CF2115-42%, Note 1
  • Tensile Modulus, SACMA SRM01R94, 0°, T1000 GB-124-36%, Note 1
  • Tensile Modulus, SACMA SRM01R94, 0° M46J-124-36%, Note 1
  • Compressive Strength, SACMA SRM01R94, 90°, M46J-124-36%, Note 1
  • Compressive Strength, SACMA SRM01R94, 90°, T1000 GB-124-36%, Note 1
  • Compressive Strength, SACMA SRM01R94, 0°, CF2115-42%, Note 1
  • Compressive Strength, SACMA SRM01R94, 90°, CF2115-42%, Note 1
  • Compressive Strength, SACMA SRM01R94, 0°, CF1218-42%, Note 1
  • Compressive Strength, SACMA SRM01R94, 90°, CF1218-42%, Note 1
  • Compressive Strength, SACMA SRM01R94, 0°, CF7234-42%, Note 1
  • Compressive Strength, SACMA SRM01R94, 90°, CF4534-42%, Note 1
  • Compressive Strength, SACMA SRM01R94, 0°, CF4534-42%, Note 1
  • Compressive Strength, SACMA SRM01R94, 90°, CF7234-42%, Note 1
  • Compressive Strength, SACMA SRM01R94, 0°, M46J-124-36%, Note 1
  • Compressive Strength, SACMA SRM01R94, 0°, T1000 GB-124-36%, Note 1
  • Compressive Modulus, SACMA SRM01R94, 90°, M46J-124-36%, Note 1
  • Compressive Modulus, SACMA SRM01R94, 90°, T1000 GB-124-36%, Note 1
  • Compressive Modulus, SACMA SRM01R94, 90°, CF1218-42%, Note 1
  • Compressive Modulus, SACMA SRM01R94, 90°, CF4534-42%, Note 1
  • Compressive Modulus, SACMA SRM01R94, 90°, CF7234-42%, Note 1
  • Compressive Modulus, SACMA SRM01R94, 0°, CF4534-42%, Note 1
  • Compressive Modulus, SACMA SRM01R94, 0°, CF1218-42%, Note 1
  • Compressive Modulus, SACMA SRM01R94, 0°, CF7234-42%, Note 1
  • Compressive Modulus, SACMA SRM01R94, 90°, CF2115-42%, Note 1
  • Compressive Modulus, SACMA SRM01R94, 0°, CF2115-42%, Note 1
  • Compressive Modulus, SACMA SRM01R94, 0°, T1000 GB-124-36%, Note 1
  • Compressive Modulus, SACMA SRM01R94, 0°, M46J-124-36%, Note 1
  • Shear Modulus, ASTM D3518, In-plane, CF1218-42%, Note 1
  • Shear Modulus, ASTM D3518, In-plane, T1000 GB-124-36%, Note 1
  • Shear Modulus, ASTM D3518, In-plane, CF4534-42%, Note 1
  • Shear Modulus, ASTM D3518, In-plane, M46J-124-36%, Note 1
  • Shear Modulus, ASTM D3518, In-plane, CF2115-42%, Note 1
  • Shear Modulus, ASTM D3518, In-plane, CF7234-42%, Note 1
  • Shear Strength, ASTM D2344, 0° Interlaminar, CF2115-42%, Note 1
  • Shear Strength, ASTM D2344, 0° Interlaminar, CF4534-42%, Note 1
  • Shear Strength, ASTM D2344, I0° Interlaminar, CF1218-42%, Note 1
  • Shear Strength, ASTM D2344, 0° Interlaminar, M46J-124-36%, Note 1
  • Shear Strength, ASTM D3518, In-plane, M46J-124-36%, Note 1
  • Shear Strength, ASTM D3518, In-plane, CF2115-42%, Note 1
  • Shear Strength, ASTM D2344, 0° Interlaminar, T1000 GB-124-36%, Note 1
  • Shear Strength, ASTM D3518, In-plane, CF4534-42%, Note 1
  • Shear Strength, ASTM D3518, In-plane, CF1218-42%, Note 1
  • Shear Strength, ASTM D3518, In-plane, T1000 GB-124-36%, Note 1
  • Shear Strength, ASTM D3518, In-plane, CF7234-42%, Note 1
  • Shear Strength, ASTM D2344, 0° Interlaminar, CF7234-42%, Note 1
  • Glass Transition Temp, Tg, DMA E' onset Tg, 1 hr at 120°C
  • Glass Transition Temp, Tg, DMA E' onset Tg, 1 hr at 135°C
  • Glass Transition Temp, Tg, DMA E' onset Tg, 1 hr at 120°C + 2 hrs at 150°C
  • Cure Time
  • Cure Time
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Solvay, former Rhodia Engineering Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.