MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
CRP  Windform
Solaxis ASA 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; ASA Polymer

Material Notes: Used to build consistently high-quality parts, with exceptional UV stability and the best aesthetics of any FDM® thermoplastic. ASA is a popular all-purpose prototyping material for users of Fortus 380mc™, 450mc™ and 900mc™ 3D Printers, and the Stratasys F123 ™ Series. ASA parts can match or exceed the mechanical properties of ABS in general prototyping uses. Its UV-resistance makes it especially suited to production parts for outdoor commercial and infrastructure use. Its wide selection of colors and matte finish makes it ideal for attractive prototypes in consumer sporting goods, tools and automotive components and accessories.

Information provided by Solaxis Ingenious Manufacturing

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Hardness, Rockwell R, ASTM D785
  • Tensile Strength, Ultimate, ASTM D638, ZX Orientation, Type 1, 0.2 in./min
  • Tensile Strength, Ultimate, ASTM D638, XZ Orientation, Type 1, 0.2 in./min
  • Tensile Strength, Yield, ASTM D638, ZX Orientation, Type 1, 0.2 in./min
  • Tensile Strength, Yield, ASTM D638, XZ Orientation, Type 1, 0.2 in./min
  • Elongation at Break, ASTM D638, ZX Orientation, Type 1, 0.2 in./min
  • Elongation at Break, ASTM D638, XZ Orientation, Type 1, 0.2 in./min
  • Elongation at Yield, ASTM D638, XZ Orientation, Type 1, 0.2 in./min
  • Elongation at Yield, ASTM D638, ZX Orientation, Type 1, 0.2 in./min
  • Tensile Modulus, ASTM D638, ZX Orientation, Type 1, 0.2 in./min
  • Tensile Modulus, ASTM D638, XZ Orientation, Type 1, 0.2 in./min
  • Flexural Strength, ASTM D790, ZX Orientation, Method 1, 0.05 in./min
  • Flexural Strength, ASTM D790, XZ Orientation, Method 1, 0.05 in./min
  • Flexural Modulus, ASTM D790, ZX Orientation, Method 1, 0.05 in./min
  • Flexural Modulus, ASTM D790, XZ Orientation, Method 1, 0.05 in./min
  • Flexural Strain at Break, ASTM D790, ZX Orientation, Method 1, 0.05 in./min
  • Izod Impact, Notched, ASTM D256, XZ orientation, Method A
  • Izod Impact, Unnotched, ASTM D256, XZ orientation, Method A
  • Volume Resistivity, ASTM D257, XZ
  • Dielectric Constant, ASTM D150-98, XZ
  • Dielectric Strength, ASTM D149-09, Method A, XZ
  • Dielectric Strength, ASTM D149-09, Method A, ZX
  • Dissipation Factor, ASTM D150-98, XZ
  • CTE, linear, Parallel to Flow, ASTM E831
  • CTE, linear, Transverse to Flow, ASTM E831
  • Deflection Temperature at 0.46 MPa (66 psi), ASTM D648
  • Deflection Temperature at 1.8 MPa (264 psi), ASTM D648
  • Vicat Softening Point, ASTM D1525, Rate B/50
  • Glass Transition Temp, Tg
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Elmet Technologies
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.