MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Abatron AboCoat 8006-3/8606-3 Clear Versatile Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy Encapsulant, Unreinforced

Material Notes: Clear epoxy protective and dielectric coatings. For spraying, brushing or rolling on metal, concrete, masonry, wood, fiberglass and most surfaces. Good adhesion, flexibility, hardness, water and chemical resistance.

Suggested Uses: Heavy-duty all-purpose protection against water, alkalis, diluted acids, common solvents, corrosion, wear. Corrosion inhibition also on tightly bound rust. Good salt spray resistance in marine and industrial applications. Concrete, wood and metal floors coating. Brushing on moist or wet surfaces tends to emulsify water, which then evaporates with solvent. Protection of wooden furniture in plants, laboratories, commercial kitchens, hospitals. Most effective for protection of all kinds of electric and electronic components.

Processing:

Ratio by volume: 1/1 AboCoat/AboCure

Cure Schedule: Room temperature cure 4-6 hours for handling, 3-4 days for full physical properties, and 6-8 days for full chemical properties. High temperature cure 25 minutes at 200°F, 15 minutes at 250°F, 10 minutes at 300°F, or 5 minutes at 350°F.

Information provided by Abatron.

Vendors:
Available Properties
  • Density
  • Solids Content, Total
  • Viscosity Measurement, secs., #4 Ford cup.
  • Film Elongation at Break, MD, Direction not specified
  • Impact Test, Forward/reverse
  • Gloss, 3 mils, 48 hours
  • Transmission, Visible, clear; thickness not quantified
  • Dry Time
  • Pot Life
  • Shelf Life
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.