MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Saint-Gobain Meldin® 2211 Bearing
Categories: Polymer; Thermoset; Polyimide, TS

Material Notes: General Notes on Meldin 2000 Series Bearing Products:
For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin® 2000 Series can be machined into various configurations, from rod or sheet stock shapes. Black in color. Meldin® 2000 Series offers very high compression strength, high creep resistance, and dimensional stability.
Specific Notes on Meldin® 2211 Bearing
Meldin® 2211 offers the balanced properties of low friction, high strength and resistance to compressive creep.

Applications include: Appliances, Automotive, Industrial, Semiconductor, Transportation.

Specification Notes: Note that the specifications given for this product are typical specifications for the Meldin® 2000 Series, and individual products will vary as indicated in the material notes.
Information provided by Saint Gobain Performance Products.

Vendors:
Available Properties
  • Specific Gravity, ASTM D792
  • Water Absorption, ASTM D570
  • Deformation, ASTM D621, 24 hrs. Mold Direction
  • Outgassing - Total Mass Loss, ASTM E595, % WVR
  • Outgassing - Total Mass Loss, ASTM E5955
  • Collected Volatile Condensable Material, ASTM E55955
  • Hardness, Shore D, ASTM D2240
  • Tensile Strength, Ultimate, ASTM D 638
  • Tensile Strength, Ultimate, ASTM D 638
  • Elongation at Break, ASTM D 638
  • Elongation at Break, ASTM D 638
  • Tensile Modulus, ASTM D 638
  • Tensile Modulus, ASTM D 638
  • Flexural Strength, ASTM D 790
  • Flexural Modulus, ASTM D 790
  • Izod Impact, Notched, ASTM D 256
  • Volume Resistivity, ASTM D257
  • Surface Resistance, ASTM D257
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dielectric Constant, ASTM D150
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • Dissipation Factor, ASTM D150
  • CTE, linear, ASTM E831-93
  • Thermal Conductivity, C518/C177
  • Maximum Service Temperature, Air, UL-746 B
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Saint Gobain Performance Plastics

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Ensinger SPI
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.