MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Rulon Bearings
Chemical Concepts Chem-Set™ RTV4500 Acetoxy cure silicone sealant
Categories: Polymer; Adhesive; Thermoset; Silicone; Silicone, RTV, Adhesive/Sealant Grade

Material Notes: Chem-Set™ RTV 4500 is a one component room temperature vulcanizing (RTV) industrial/construction grade silicone sealant and adhesive that has been chemically formulated for high strength adhesion. When fully cured, this unique VOC compliant formula offers UV stability and excellent adhesion to form waterproof and airtight bonds to metal, steel, tile, fiberglass, ceramic, glass, aluminum, painted surfaces, wood, plywood, marble, plus many other common substrates.

This product is offers all weather performance to meets Green Building Standards. Features and Benefits: High Strength, Excellent Weatherability, UV Stable, Non-Yellowing, VOC Compliant, Non-Flammable, Waterproof , Excellent Adhesion, Non-Shrinking, Construction & Industrial Applications: Kitchen And Bath, Countertops/Backsplashes, Sealing & Glazing, HVAC/R , Plumbing, Roofing, Sanitary Seals, Precast Concrete, Transportation Seals, Marine Cabins, Appliance Trim, Interior/Exterior, Above Grade.

Information provided by Chemical Concepts™.

Vendors:
Available Properties
  • Specific Gravity, 50% RH
  • Volatile Organic Compounds (VOC) Content
  • Hardness, Shore A, ASTM C661, Tested at 77°F & 50% RH
  • Tensile Strength, ASTM D412, Tested at 77°F & 50% RH
  • Elongation at Break, ASTM D412, Tested at 77°F & 50% RH
  • Dielectric Constant, Tested at 77°F & 50% RH
  • Dielectric Strength, Tested at 77°F & 50% RH
  • Maximum Service Temperature, Air
  • Maximum Service Temperature, Air, intermittent
  • Minimum Service Temperature, Air
  • Extrusion Rate, ASTM C 1183, 1/8" orifice @ 50 psi, modified.
  • Shelf Life, Tested at 77°F & 50% RH
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
none

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Aluminum Castings
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.