MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  
Metal adhesives
Master Bond EP38FLAO Two Component Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive; Epoxy Encapsulant, Unreinforced; Epoxy, Thermally Conductive

Material Notes: Key Features:
  • Thermally conductive
  • Electrically insulative
  • High flexibility
  • Very long open time
  • Cures at room or elevated temperatures
  • Excellent flowability
Product Description: Master Bond EP38FLAO is a versatile two component thermally conductive, electrically insulating epoxy. This epoxy can be used for high performance bonding, sealing, coating, potting and encapsulation. This system features a convenient and forgiving one to one mix ratio by weight or volume. It has an exceptionally long working life as well. This in and of itself is highly attractive, but add to this that it is a lower exotherm system with splendid flow, which enables it to be used in all kinds of potting and encapsulation applications, particularly those that are larger in size. Also noteworthy are its outstanding thermal conductivity, superior electrical insulation properties along with a substantial degree of flexibility. Its top notch flexibility allows it to withstand rigorous thermal cycling as well as mechanical and thermal shocks. EP38FLAO bonds well to a wide variety of substrates such as metals, glass, ceramics, composites, many rubbers and plastics, and is an excellent adhesive. It has reasonably good chemical resistance to water, oils and many fuels. It has a wide service temperature range of -100°F to 250°F. Parts A and B are off white in color. This multifaceted system is widely used in the electronic, electrical, computer, aerospace, opto-electronic and specialty OEM applications where electrical insulation and heat transfer are required and excellent flow properties are desirable. EP38FLAO is particularly special because it possesses a high level of flexibility and thermal conductivity while it retains the desirable physical characteristics inherent in epoxies.

Product Advantages:

  • Convenient mixing: easy to use, non-critical one to one mix ratio by weight or volume
  • High thermal conductivity with striking electrical insulation properties
  • Superior bond strength to a wide variety of substrates
  • Low exotherm and a long working life
  • Excellent flowability well suited for all kinds of potting and encapsulations
  • Capable of withstanding rigorous thermal cycling and shocks

Information provided by Master Bond Inc.

Vendors:
Available Properties
  • Viscosity, Part B
  • Viscosity, mixed
  • Viscosity, Part A
  • Hardness, Shore A
  • Hardness, Shore D
  • Tensile Strength
  • Adhesive Bond Strength, Tensile lap, Aluminum to Aluminum
  • Peel Strength
  • Volume Resistivity
  • Dielectric Constant
  • Dielectric Strength
  • CTE, linear
  • Thermal Conductivity
  • Maximum Service Temperature, Air
  • Minimum Service Temperature, Air
  • Cure Time
  • Cure Time
  • Working Life, After mixing, 100 g batch
  • Shelf Life, in original, unopened containers
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

Manufacturer Notes:
Master Bond Inc.

Category Notes
Plastic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

 

Metal adhesives
Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.