MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultrason® KR 4113 PESU with 10/10% Carbon Fibers/Graphite and 10% PTFE
Categories: Polymer; Thermoplastic; Polyethersulfone (PES); Polyethersulfone (PES), PTFE Filled; Polyethersulfone, Carbon Fiber Reinforced; Polyethersulfone, Mineral Reinforced

Material Notes: Description: Compound based on PES with 30 % filler. The filler system, a mixture of carbon fibers, graphite and PTFE powder, considerably improves Ultrason’s tribological properties. In addition, this product has a very small expansion coefficient and low tendency to swell in hot oils. Abbreviated designation according to ISO 1043-1: PESU-(CF+ZD)

Typical applications: Oil control piston in standard automotive oil pumps and oil control piston in volume controlled automotive oil-pumps

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.700 - 0.800 g/cc0.0253 - 0.0289 lb/in³
Density 1.48 g/cc0.0535 lb/in³ISO 1183
Water Absorption 1.5 %1.5 %ISO 62
Moisture Absorption at Equilibrium 0.50 %0.50 %23°C; 50% RH; ISO 62
Viscosity Test 56 cm³/g0.56 dl/gISO 307
Linear Mold Shrinkage, Flow 0.0031 cm/cm0.0031 in/inISO 2577, 294-4
Linear Mold Shrinkage, Transverse 0.0046 cm/cm0.0046 in/inISO 2577, 294-4
Melt Flow 14.8 g/10 min
@Load 10.0 kg,
Temperature 360 °C
14.8 g/10 min
@Load 22.0 lb,
Temperature 680 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 180 MPa
@Load 98.0 kg,
Time 30.0 sec
26100 psi
@Load 216 lb,
Time 0.00833 hour
ISO 2039-1
Tensile Strength  108 MPa
@Treatment Temp. 150 °C,
Time 7.20e+6 sec
15700 psi
@Treatment Temp. 302 °F,
Time 2000 hour
used oil
 108 MPa
@Treatment Temp. 150 °C,
Time 1.08e+7 sec
15700 psi
@Treatment Temp. 302 °F,
Time 3000 hour
used oil
 109 MPa
@Treatment Temp. 150 °C,
Time 7.20e+6 sec
15800 psi
@Treatment Temp. 302 °F,
Time 2000 hour
new oil
 109 MPa
@Treatment Temp. 150 °C,
Time 3.60e+6 sec
15800 psi
@Treatment Temp. 302 °F,
Time 1000 hour
used oil
 110 MPa
@Treatment Temp. 150 °C,
Time 3.60e+6 sec
16000 psi
@Treatment Temp. 302 °F,
Time 1000 hour
new oil
 111.0 MPa
@Treatment Temp. 150 °C,
Time 1.08e+7 sec
16100 psi
@Treatment Temp. 302 °F,
Time 3000 hour
new oil
 112 MPa
@Treatment Temp. 150 °C,
Time 0.000 sec
16200 psi
@Treatment Temp. 302 °F,
Time 0.000 hour
new oil
 112 MPa
@Treatment Temp. 150 °C,
Time 0.000 sec
16200 psi
@Treatment Temp. 302 °F,
Time 0.000 hour
used oil
Tensile Strength, Yield 105 MPa15200 psi50mm/min; ISO 527-1/-2
Elongation at Yield 1.3 %1.3 %50mm/min; ISO 527-1/-2
Tensile Modulus 10.1 GPa1460 ksiISO 527-1/-2
Izod Impact, Notched (ISO) 5.00 kJ/m²
@Temperature 23.0 °C
2.38 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched 1.90 J/cm²
@Temperature 23.0 °C
9.04 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.300 J/cm²
@Temperature -30.0 °C
1.43 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.450 J/cm²
@Temperature 23.0 °C
2.14 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 8500 ohm-cm8500 ohm-cmIEC 60093
Surface Resistance 4000 ohm4000 ohmIEC 60093
Dielectric Strength 8.00 kV/mm203 kV/inDIN 53752
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow  11.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
6.11 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 75-1/-2
 13.0 µm/m-°C
@Temperature 180 °C
7.22 µin/in-°F
@Temperature 356 °F
DIN 53752
 26.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 25.0 °C
14.4 µin/in-°F
@Thickness 0.157 in,
Temperature 77.0 °F
 26.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 75.0 °C
14.4 µin/in-°F
@Thickness 0.157 in,
Temperature 167 °F
 27.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 125 °C
15.0 µin/in-°F
@Thickness 0.157 in,
Temperature 257 °F
 27.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 175 °C
15.0 µin/in-°F
@Thickness 0.157 in,
Temperature 347 °F
 33.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 25.0 °C
18.3 µin/in-°F
@Thickness 0.0787 in,
Temperature 77.0 °F
 33.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 75.0 °C
18.3 µin/in-°F
@Thickness 0.0787 in,
Temperature 167 °F
 34.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 125 °C
18.9 µin/in-°F
@Thickness 0.0787 in,
Temperature 257 °F
CTE, linear, Transverse to Flow  19.5 µm/m-°C
@Thickness 2.00 mm,
Temperature 125 °C
10.8 µin/in-°F
@Thickness 0.0787 in,
Temperature 257 °F
 20.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 75.0 °C
11.1 µin/in-°F
@Thickness 0.0787 in,
Temperature 167 °F
 20.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 25.0 °C
11.1 µin/in-°F
@Thickness 0.0787 in,
Temperature 77.0 °F
 23.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 75.0 °C
12.8 µin/in-°F
@Thickness 0.157 in,
Temperature 167 °F
 24.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 125 °C
13.3 µin/in-°F
@Thickness 0.157 in,
Temperature 257 °F
 24.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 25.0 °C
13.3 µin/in-°F
@Thickness 0.157 in,
Temperature 77.0 °F
 25.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 175 °C
13.9 µin/in-°F
@Thickness 0.157 in,
Temperature 347 °F
Deflection Temperature at 1.8 MPa (264 psi) 220 °C428 °FISO 75-1/-2
Glass Transition Temp, Tg 225 °C437 °FISO 11357-1/-2
Decomposition Temperature >= 400 °C>= 752 °F
Ignition Temperature >= 500 °C>= 932 °FASTM D1929
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FHopper throat
Zone 1 350 °C662 °FFeed zone
Zone 2 360 °C680 °FCompression
Zone 3 370 °C698 °FMetering-zone
Zone 4 370 °C698 °FNozzle
Melt Temperature 350 - 390 °C662 - 734 °FInjection molding/extrusion
 370 °C698 °FOptimal
Mold Temperature 150 - 190 °C302 - 374 °FInjection molding
 170 °C338 °FOptimal
Drying Temperature 140 °C284 °F
Dry Time 4 hour4 hour
 
Descriptive Properties
ColorBlack
Commercial StatusEurope
Primary Processing TechniqueInjection molding and Extrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Thiodiglycol HP
BASF Ultrason® E 1010 PES
BASF Ultrason® E 2010 G4 MR SW 15102 20% Glass Filled PESU
BASF Ultrason® S 2010 G4 20% Glass Filled PSU
BASF Basantol® 215 Yellow Liquid

PBASG0171 / 131804

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.