MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Abatron AboCast 50-3/AboCure 50-12 Epoxy
Categories: Polymer; Adhesive; Thermoset; Epoxy

Material Notes: Data provided by the manufacturer, Abatron, Inc. Light motor oil viscosity, almost colorless. Shelf life is 12+ months.

Key Words: potting, casting, encapsulating, impregnating
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 1.0 cP1.0 cP50-12 water-like viscosity
 11000 - 14000 cP11000 - 14000 cP50-3
 2250 cP
@Temperature 25.0 °C
2250 cP
@Temperature 77.0 °F
at 100/13 (50-3/50-12) pbw
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 106106
Tensile Strength, Ultimate 78.6 MPa11400 psi
Elongation at Break 4.4 %4.4 %
Flexural Yield Strength 95.83 MPa13900 psi
Flexural Modulus 3.00 GPa435 ksi
Compressive Yield Strength 112.38 MPa16299 psi
Compressive Modulus 3.03 GPa440 ksi
Izod Impact, Notched 0.267 J/cm0.500 ft-lb/in
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 6.10e+15 ohm-cm6.10e+15 ohm-cm
Surface Resistance 7.85e+15 ohm7.85e+15 ohm
Dielectric Constant  3.42
@Frequency 1e+6 Hz
3.42
@Frequency 1e+6 Hz
 3.9
@Frequency 1000 Hz
3.9
@Frequency 1000 Hz
 4.02
@Frequency 60 Hz
4.02
@Frequency 60 Hz
Dissipation Factor  0.0074
@Frequency 60 Hz
0.0074
@Frequency 60 Hz
 0.020
@Frequency 1000 Hz
0.020
@Frequency 1000 Hz
 0.032
@Frequency 1e+6 Hz
0.032
@Frequency 1e+6 Hz
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 111 °C232 °FDeflection temperature; load unknown.
 
Processing PropertiesMetricEnglishComments
Pot Life 30 min30 min500 g
 
Descriptive Properties
Exotherm255°CPeak

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Akro-Plastic Akromid® A3 1 L black (4652) PA 66 + PP Dry
Abatron AboCast 8504-5 One-Component Epoxy
Devcon Zip Patch™ Epoxy
Devcon Underwater Repair Putty (UW) Epoxy
Bakelite® EP 8414 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage

PABDI1 / 21988

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.