MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.

Benefits: This product offers excellent flame retardancy properties (UL 94, GWIT) combined with excellent processing, mechanical and electrical performance.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: This product is ideally suited for appliance and industrial control applications such as switches, timers and contactors.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³ISO 1183/A
Water Absorption 0.80 %
@Temperature 23.0 °C,
Time 86400 sec
0.80 %
@Temperature 73.4 °F,
Time 24.0 hour
ISO 62
Viscosity  70 cP
@Shear Rate 100 1/s,
Temperature 300 °C
70 cP
@Shear Rate 100 1/s,
Temperature 572 °F
 105 cP
@Shear Rate 100 1/s,
Temperature 290 °C
105 cP
@Shear Rate 100 1/s,
Temperature 554 °F
 120 cP
@Shear Rate 100 1/s,
Temperature 280 °C
120 cP
@Shear Rate 100 1/s,
Temperature 536 °F
Linear Mold Shrinkage 0.0063 cm/cm0.0063 in/inIsotropy
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/in
Linear Mold Shrinkage, Transverse 0.0095 cm/cm0.0095 in/in
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 130 MPa18900 psiISO 527 Type 1A
 140 MPa20300 psiASTM D638
Tensile Stress at Strain  45.0 MPa
@Strain 0.5 %
6530 psi
@Strain 0.5 %
 75.0 MPa
@Strain 1.5 %
10900 psi
@Strain 1.5 %
 80.0 MPa
@Strain 1 %
11600 psi
@Strain 1 %
Elongation at Break 2.2 %2.2 %ISO 527 Type 1A
 2.5 %2.5 %ASTM D638
Tensile Modulus 10.0 GPa1450 ksiISO 527 Type 1A
Flexural Strength 200 MPa29000 psiISO 178
 200 MPa29000 psiASTM D790
Flexural Modulus 9.50 GPa1380 ksiISO 178
 9.50 GPa1380 ksiASTM D790
Izod Impact, Notched 1.15 J/cm2.15 ft-lb/inASTM D256
Izod Impact, Notched (ISO) 10.0 kJ/m²4.76 ft-lb/in²ISO 180/1eA
Charpy Impact Unnotched 4.20 J/cm²20.0 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.950 J/cm²4.52 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant 3.33.3IEC 60250
Dielectric Strength 42.0 kV/mm1070 kV/inIEC 60243
Dissipation Factor 0.0100.010IEC 60250
Comparative Tracking Index 400 V400 VSolution B; IEC 60112
 450 V450 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 263 °C505 °FISO 11357
Deflection Temperature at 1.8 MPa (264 psi) 226 °C439 °FISO 75/Af
UL RTI, Electrical  130 °C
@Thickness 0.750 mm
266 °F
@Thickness 0.0295 in
 130 °C
@Thickness 1.50 mm
266 °F
@Thickness 0.0591 in
 130 °C
@Thickness 3.00 mm
266 °F
@Thickness 0.118 in
UL RTI, Mechanical with Impact  90.0 °C
@Thickness 0.750 mm
194 °F
@Thickness 0.0295 in
 100 °C
@Thickness 1.50 mm
212 °F
@Thickness 0.0591 in
 100 °C
@Thickness 3.00 mm
212 °F
@Thickness 0.118 in
Flammability, UL94  V-0
@Thickness 0.800 mm
V-0
@Thickness 0.0315 in
1210
 V-0
@Thickness 1.60 mm
V-0
@Thickness 0.0630 in
1210
 V-0
@Thickness 3.20 mm
V-0
@Thickness 0.126 in
1210
Oxygen Index 31 %31 %ISO 4589
Glow Wire Ignition Temperature  800 °C
@Thickness 0.800 mm
1470 °F
@Thickness 0.0315 in
ISO 60695-2-13
 825 °C
@Thickness 1.60 mm
1520 °F
@Thickness 0.0630 in
ISO 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
ISO 60695-2-12
 960 °C
@Thickness 1.60 mm
1760 °F
@Thickness 0.0630 in
ISO 60695-2-12
 960 °C
@Thickness 3.20 mm
1760 °F
@Thickness 0.126 in
ISO 60695-2-12
 
Processing PropertiesMetricEnglishComments
Feed Temperature 270 - 280 °C518 - 536 °F
Mold Temperature 70.0 - 100 °C158 - 212 °F
Drying Temperature 80.0 °C176 °F
Moisture Content <= 0.20 %<= 0.20 %
 
Descriptive Properties
Compression Zone275-285°C
Fire and smoke F indexI3/F3NF F 16 101
Mixing Zone280-290°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, Conditioned
EMS-Grivory Grilamid® 2D 20 nat PA612
Avient Lubri-Tech™ NN-30GF/15T HS FR Nylon 6/6, Glass Filled
Domo TECHNYL® A 218 PA66, 33% glass fiber, DRY
Azoty Tarnow™ Tarnamid® T-27 MCS V0 Polyamide 6 - Flame Retarded, Unreinforced

PRHOD706 / 137937

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.