MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Domo TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 30% Glass Fiber Filled

Material Notes: Description: TECHNYL® A 30H1 V30 is a brominated flame retardant polyamide 66, reinforced with 30% of glass fiber, for injection molding. This product is available in natural & black color.

Benefits: This product offers excellent flame retardancy properties (UL 94, GWIT) combined with excellent processing, mechanical and electrical performance.

Available in: Asia Pacific, Europe, Latin America and North America

Regulations compliance: Grades produced or imported in Europe comply with directive 453/2010/EC, which amends REACH directive 1907/2006/EC. This grade complies with RoHS directive 2002/95/EC. Unless specified, this grade is not suitable for food contact, medical devices or toy applications.

Applications: This product is ideally suited for appliance and industrial control applications such as switches, timers and contactors.

DOMO Chemicals has acquired Solvay’s Performance Polyamides Business in Europe.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.57 g/cc0.0567 lb/in³ISO 1183/A
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 95.0 MPa13800 psiISO 527 Type 1A
Elongation at Break 3.5 %3.5 %ISO 527 Type 1A
Tensile Modulus 7.00 GPa1020 ksiISO 527 Type 1A
Flexural Strength 170 MPa24700 psiISO 178
Flexural Modulus 7.00 GPa1020 ksiISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²6.19 ft-lb/in²ISO 180/1eA
Charpy Impact Unnotched 5.00 J/cm²23.8 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 1.20 J/cm²5.71 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 3.63.6IEC 60250
Dielectric Strength 40.0 kV/mm1020 kV/inIEC 60243
Dissipation Factor 0.0500.050IEC 60250
Comparative Tracking Index 500 V500 VSolution B; IEC 60112
 600 V600 VSolution A; IEC 60112
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.20 %<= 0.20 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Domo TECHNYL® A 30 H1 V30 PA66, 30% glass fiber, DRY
Mitsubishi Chemical Advanced Materials Nylatron™ GF30 / Ertalon™ 66 GF30 PA66 30% glass filled, extruded
Domo Technyl® C216V15 15% Glass Filled Nylon 6
Domo TECHNYL® C 548B V15 Black PA6, 15% glass filled, DRY
Domo TECHNYL® C 246SI V11 PA6, 11% glass filled, DRY

PRHOD707 / 137938

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.