MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

AISI 3140
Categories: Metal; Ferrous Metal; Alloy Steel; Low Alloy Steel; Carbon Steel; Medium Carbon Steel

Material Notes: A medium carbon low alloy steel.

Key Words: AISI 3140, UNS G31400, SAE 3140 (obsolete), SAE J775(93), ASTM A519(96)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 7.85 g/cc0.284 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 790 MPa115000 psiASTM D638
Tensile Strength, Yield 520 MPa75400 psiASTM D638
Elongation at Break 25 %25 %ASTM D638
Machinability 55 %55 %as compared to AISI 1112 steel with a machinability rating of 100.
 
Component Elements PropertiesMetricEnglishComments
Carbon, C 0.38 - 0.43 %0.38 - 0.43 %
Chromium, Cr 0.55 - 0.75 %0.55 - 0.75 %
Iron, Fe 96.1 - 97.1 %96.1 - 97.1 %as balance
Manganese, Mn 0.70 - 0.90 %0.70 - 0.90 %
Nickel, Ni 1.1 - 1.4 %1.1 - 1.4 %
Phosphorus, P <= 0.040 %<= 0.040 %
Silicon, Si 0.15 - 0.35 %0.15 - 0.35 %
Sulfur, S <= 0.040 %<= 0.040 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Low Alloy Steel
AISI 4140 Steel, annealed at 815°C (1500°F) furnace cooled 11°C (20°F)/hour to 665°C (1230°F), air cooled, 25 mm (1 in.) round
AISI 4140 Steel, normalized at 870°C (1600°F), air cooled, 100 mm (4 in.) round
Overview of materials for AISI 4000 Series Steel
AISI 1330 Steel

M3140A / 7424

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.