MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultradur® S 4090 G6X 30% Glass Filled PBT + ASA
Categories: Polymer; Thermoplastic; ASA Polymer; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + ASA Blend, Glass Fiber Reinforced

Material Notes: PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 30% of glass fibers for industrial parts with high dimensional stability, for example internal components for vehicles, plug connectors and housings.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.47 g/cc0.0531 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %23°C; 50% RH
Water Absorption at Saturation 0.40 %0.40 %DIN 53495/1L
Viscosity Measurement  70
@Temperature 290 °C
70
@Temperature 554 °F
20 mins plasticating
 75
@Temperature 300 °C
75
@Temperature 572 °F
10 mins plasticating
 75
@Temperature 280 °C
75
@Temperature 536 °F
30 mins plasticating
 90
@Temperature 270 °C
90
@Temperature 518 °F
30 mins plasticating
 95
@Temperature 290 °C
95
@Temperature 554 °F
10 mins plasticating
 100
@Temperature 300 °C
100
@Temperature 572 °F
5 mins plasticating
 100
@Temperature 260 °C
100
@Temperature 500 °F
30 mins plasticating
 105
@Temperature 280 °C
105
@Temperature 536 °F
10 mins plasticating
 106
@Temperature 250 °C
106
@Temperature 482 °F
30 mins plasticating
 110
@Temperature 270 °C
110
@Temperature 518 °F
10 mins plasticating
 115
@Temperature 260 °C
115
@Temperature 500 °F
10 mins plasticating
 115
@Temperature 240 °C
115
@Temperature 464 °F
30 mins plasticating
 117
@Temperature 250 °C
117
@Temperature 482 °F
10 mins plasticating
 120
@Temperature 240 °C
120
@Temperature 464 °F
10 mins plasticating
Viscosity Test 104 cm³/g1.04 dl/gViscosity number; ISO 1628
Linear Mold Shrinkage, Flow 0.0016 cm/cm0.0016 in/inSheet
 0.0029 cm/cm0.0029 in/in60x60x2 mm; ISO 294
Linear Mold Shrinkage, Transverse 0.0082 cm/cm0.0082 in/in60x60x2 mm; ISO 294
 0.0095 cm/cm0.0095 in/inSheet
Melt Flow 29.4 g/10 min
@Load 2.16 kg,
Temperature 275 °C
29.4 g/10 min
@Load 4.76 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 132 MPa19100 psi50 mm/min; ISO 527-2
Elongation at Yield 2.5 %2.5 %50 mm/min; ISO 527-2
Modulus of Elasticity 9.80 GPa1420 ksiISO 527-2
Flexural Strength 190 MPa27600 psiISO 178
Charpy Impact Unnotched  5.50 J/cm²
@Temperature -30.0 °C
26.2 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 6.40 J/cm²
@Temperature 23.0 °C
30.5 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²23; ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.50e+15 ohm-cm1.50e+15 ohm-cmIEC 93
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 93
Dielectric Constant  3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
IEC 250
 3.9
@Frequency 100 Hz
3.9
@Frequency 100 Hz
IEC 250
Dielectric Strength 41.0 kV/mm1040 kV/inIEC 243/1
Dissipation Factor  0.0046
@Frequency 100 Hz
0.0046
@Frequency 100 Hz
IEC 250
 0.0202
@Frequency 1e+6 Hz
0.0202
@Frequency 1e+6 Hz
IEC 250
Comparative Tracking Index 425 V425 VTest solution A; IEC 112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 30.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
16.7 µin/in-°F
@Temperature 73.4 - 176 °F
DIN 53752
Melting Point 220 - 225 °C428 - 437 °FDSC; ISO 11357-3
Maximum Service Temperature, Air 170 °C338 °F
Deflection Temperature at 0.46 MPa (66 psi) 220 °C428 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 205 °C401 °FISO 75-2
Flammability, UL94 HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Diameter 0.800 mm
HB
@Diameter 0.0315 in
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FHopper Throat
Zone 1 260 °C500 °FFeeding zone
Zone 2 265 °C509 °FCompression
Zone 3 270 °C518 °FMetering-zone
Zone 4 270 °C518 °FNozzle
Melt Temperature >= 260 °C>= 500 °FInjection-molding
 270 °C518 °Ffor shrinkage test, Optimal
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
 80.0 °C176 °Ffor shrinkage test, Optimal
Drying Temperature 80.0 - 120 °C176 - 248 °F
Dry Time 4 hour4 hour
 
Descriptive Properties
ColorNatural and Black
Commercial StatusEurope
Peripheral Screw Speed< 0.25 m/s
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultradur® S 4090 G4X 20% Glass Filled PBT + ASA
Dow LIGHTER™ C93 Polyethylene Terephthalate (PET) Resin
BASF Ultradur® B 2300 G6 HR BK15116 30% Glass Filled PBT
Evonik Vestodur® GF 30 30% Glass Reinforced PBT
BASF Petra® 130 30% Glass Filled PET

PBASG0100 / 131734

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.