MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultradur® S 4090 G4X 20% Glass Filled PBT + ASA
Categories: Polymer; Thermoplastic; ASA Polymer; Polyester, TP; Polybutylene Terephthalate (PBT); PBT + ASA Blend, Glass Fiber Reinforced

Material Notes: PBT + ASA, low-warpage, free-flowing injection-molding grades with very good processing capabilities, containing 20% of glass fibers for industrial parts with high dimensional stability, for example internal components for vehicles, plug connectors and housings.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.39 g/cc0.0502 lb/in³ISO 1183
Moisture Absorption at Equilibrium 0.20 %0.20 %23°C; 50% RH
Water Absorption at Saturation 0.40 %0.40 %DIN 53495/1L
Viscosity Test 104 cm³/g1.04 dl/gViscosity number; ISO 1628
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inSheet
 0.0046 cm/cm0.0046 in/in60x60x2 mm; ISO 294
Linear Mold Shrinkage, Transverse 0.0091 cm/cm0.0091 in/in60x60x2 mm; ISO 294
 0.010 cm/cm0.010 in/inSheet
Melt Flow 41.7 g/10 min
@Load 2.16 kg,
Temperature 275 °C
41.7 g/10 min
@Load 4.76 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 100 MPa14500 psi50 mm/min; ISO 527-2
Elongation at Yield 2.6 %2.6 %50 mm/min; ISO 527-2
Modulus of Elasticity 6.80 GPa986 ksiISO 527-2
Charpy Impact Unnotched 4.90 J/cm²23.3 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.660 J/cm²3.14 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Melting Point 220 - 225 °C428 - 437 °FDSC; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 210 °C410 °FISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 190 °C374 °FISO 75-2
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 280 °C500 - 536 °FInjection-molding
 270 °C518 °Ffor shrinkage test
Mold Temperature 60.0 - 80.0 °C140 - 176 °F
 80.0 °C176 °Ffor shrinkage test
 
Descriptive Properties
ColorNatural and Black
Commercial StatusEurope
Primary Processing TechniqueInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultradur® S 4090 G6X 30% Glass Filled PBT + ASA
Celanese Crastin® LW9020 BK580 PBT+ASA-GF20
BASF Ultradur® S 4090 G6 High Speed 30% Glass Filled PBT + ASA
Trinseo PULSE™ 2000 EZ PC/ABS Engineering Resin
BASF Ultradur® B 4040 G4 20% Glass Filled PBT + PET

PBASG0099 / 131733

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.