MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Rynite® GW520CS NC010 Polyethylene Terephthalate (PET)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant

Material Notes: 20% Glass Reinforced Flame Retardant Polyethylene Terephthalate with Improved Glow Wire Performance

Rynite GW520CS NC010 is a 20% glass fiber reinforced flame retardant color stabilized modified polyethylene terephthalate resin.

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.61 g/cc0.0582 lb/in³ISO 1183
Melt Flow 17 g/10 min
@Load 2.16 kg,
Temperature 280 °C
17 g/10 min
@Load 4.76 lb,
Temperature 536 °F
cm³/10min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 145 MPa21000 psiISO 527-1/-2
Tensile Stress at Strain  6.65 MPa
@Strain 0.19 %,
Temperature 150 °C
965 psi
@Strain 0.19 %,
Temperature 302 °F
ISO 11403-1 -2
 11.36 MPa
@Strain 0.23 %,
Temperature 90.0 °C
1648 psi
@Strain 0.23 %,
Temperature 194 °F
ISO 11403-1 -2
 30.76 MPa
@Strain 1.22 %,
Temperature 150 °C
4461 psi
@Strain 1.22 %,
Temperature 302 °F
ISO 11403-1 -2
 34.55 MPa
@Strain 0.79 %,
Temperature 90.0 °C
5011 psi
@Strain 0.79 %,
Temperature 194 °F
ISO 11403-1 -2
 42.36 MPa
@Strain 0.52 %,
Temperature 40.0 °C
6144 psi
@Strain 0.52 %,
Temperature 104 °F
ISO 11403-1 -2
 43.13 MPa
@Strain 2.19 %,
Temperature 150 °C
6255 psi
@Strain 2.19 %,
Temperature 302 °F
ISO 11403-1 -2
 51.11 MPa
@Strain 3.27 %,
Temperature 150 °C
7413 psi
@Strain 3.27 %,
Temperature 302 °F
ISO 11403-1 -2
 52.15 MPa
@Strain 1.35 %,
Temperature 90.0 °C
7564 psi
@Strain 1.35 %,
Temperature 194 °F
ISO 11403-1 -2
 60.93 MPa
@Strain 7.09 %,
Temperature 150 °C
8837 psi
@Strain 7.09 %,
Temperature 302 °F
ISO 11403-1 -2
 66.32 MPa
@Strain 0.77 %,
Temperature 23.0 °C
9619 psi
@Strain 0.77 %,
Temperature 73.4 °F
ISO 11403-1 -2
 66.64 MPa
@Strain 1.97 %,
Temperature 90.0 °C
9665 psi
@Strain 1.97 %,
Temperature 194 °F
ISO 11403-1 -2
 68.3 MPa
@Strain 0.9 %,
Temperature 40.0 °C
9910 psi
@Strain 0.9 %,
Temperature 104 °F
ISO 11403-1 -2
 77.0 MPa
@Strain 0.86 %,
Temperature -20.0 °C
11200 psi
@Strain 0.86 %,
Temperature -4.00 °F
ISO 11403-1 -2
 77.04 MPa
@Strain 0.88 %,
Temperature 0.000 °C
11170 psi
@Strain 0.88 %,
Temperature 32.0 °F
ISO 11403-1 -2
 91.1 MPa
@Strain 1.32 %,
Temperature 40.0 °C
13200 psi
@Strain 1.32 %,
Temperature 104 °F
ISO 11403-1 -2
 101.52 MPa
@Strain 1.3 %,
Temperature 23.0 °C
14724 psi
@Strain 1.3 %,
Temperature 73.4 °F
ISO 11403-1 -2
 108.6 MPa
@Strain 1.76 %,
Temperature 40.0 °C
15750 psi
@Strain 1.76 %,
Temperature 104 °F
ISO 11403-1 -2
 121.11 MPa
@Strain 1.73 %,
Temperature 23.0 °C
17566 psi
@Strain 1.73 %,
Temperature 73.4 °F
ISO 11403-1 -2
 123.93 MPa
@Strain 1.55 %,
Temperature 0.000 °C
17975 psi
@Strain 1.55 %,
Temperature 32.0 °F
ISO 11403-1 -2
 133.42 MPa
@Strain 1.65 %,
Temperature -20.0 °C
19351 psi
@Strain 1.65 %,
Temperature -4.00 °F
ISO 11403-1 -2
 142.03 MPa
@Strain 2.35 %,
Temperature 23.0 °C
20600 psi
@Strain 2.35 %,
Temperature 73.4 °F
ISO 11403-1 -2
 145.58 MPa
@Strain 1.98 %,
Temperature 0.000 °C
21115 psi
@Strain 1.98 %,
Temperature 32.0 °F
ISO 11403-1 -2
 157.63 MPa
@Strain 2.1 %,
Temperature -20.0 °C
22862 psi
@Strain 2.1 %,
Temperature -4.00 °F
ISO 11403-1 -2
 167.5 MPa
@Strain 2.61 %,
Temperature 0.000 °C
24290 psi
@Strain 2.61 %,
Temperature 32.0 °F
ISO 11403-1 -2
Elongation at Break 2.5 %2.5 %ISO 527-1/-2
Tensile Modulus 9.00 GPa1310 ksiISO 527-1/-2
 3.013 GPa
@Temperature 150 °C
437.0 ksi
@Temperature 302 °F
ISO 11403-1 -2
 6.316 GPa
@Temperature 60.0 °C
916.1 ksi
@Temperature 140 °F
ISO 11403-1 -2
 9.165 GPa
@Temperature -20.0 °C
1329 ksi
@Temperature -4.00 °F
ISO 11403-1 -2
Secant Modulus  4.66 GPa
@Strain 2.83 %,
Temperature 40.0 °C
675 ksi
@Strain 2.83 %,
Temperature 104 °F
ISO 11403-1 -2
 5.52 GPa
@Strain 2.72 %,
Temperature 23.0 °C
801 ksi
@Strain 2.72 %,
Temperature 73.4 °F
ISO 11403-1 -2
 5.72 GPa
@Strain 2.07 %,
Temperature 40.0 °C
829 ksi
@Strain 2.07 %,
Temperature 104 °F
ISO 11403-1 -2
 6.51 GPa
@Strain 2.03 %,
Temperature 23.0 °C
945 ksi
@Strain 2.03 %,
Temperature 73.4 °F
ISO 11403-1 -2
 6.61 GPa
@Strain 1.48 %,
Temperature 40.0 °C
959 ksi
@Strain 1.48 %,
Temperature 104 °F
ISO 11403-1 -2
 7.12 GPa
@Strain 2.13 %,
Temperature 0.000 °C
1030 ksi
@Strain 2.13 %,
Temperature 32.0 °F
ISO 11403-1 -2
 7.29 GPa
@Strain 2.26 %,
Temperature -20.0 °C
1060 ksi
@Strain 2.26 %,
Temperature -4.00 °F
ISO 11403-1 -2
 7.59 GPa
@Strain 0.9 %,
Temperature 40.0 °C
1100 ksi
@Strain 0.9 %,
Temperature 104 °F
ISO 11403-1 -2
 7.81 GPa
@Strain 1.3 %,
Temperature 23.0 °C
1130 ksi
@Strain 1.3 %,
Temperature 73.4 °F
ISO 11403-1 -2
 8.00 GPa
@Strain 1.55 %,
Temperature 0.000 °C
1160 ksi
@Strain 1.55 %,
Temperature 32.0 °F
ISO 11403-1 -2
 8.09 GPa
@Strain 1.65 %,
Temperature -20.0 °C
1170 ksi
@Strain 1.65 %,
Temperature -4.00 °F
ISO 11403-1 -2
 8.15 GPa
@Strain 0.52 %,
Temperature 40.0 °C
1180 ksi
@Strain 0.52 %,
Temperature 104 °F
ISO 11403-1 -2
 8.61 GPa
@Strain 0.77 %,
Temperature 23.0 °C
1250 ksi
@Strain 0.77 %,
Temperature 73.4 °F
ISO 11403-1 -2
 8.75 GPa
@Strain 0.88 %,
Temperature 0.000 °C
1270 ksi
@Strain 0.88 %,
Temperature 32.0 °F
ISO 11403-1 -2
 8.95 GPa
@Strain 0.86 %,
Temperature -20.0 °C
1300 ksi
@Strain 0.86 %,
Temperature -4.00 °F
ISO 11403-1 -2
Charpy Impact Unnotched 3.00 J/cm²14.3 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.900 J/cm²4.28 ft-lb/in²ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance 1.00e+15 ohm1.00e+15 ohmIEC 60093
Dielectric Strength 22.0 kV/mm559 kV/inIEC 60243-1
Comparative Tracking Index 125 V125 VIEC 60112
 200 V200 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Melting Point 251 °C484 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 1.8 MPa (264 psi) 232 °C450 °FISO 75-1/-2
Flammability, UL94  V-2
@Thickness 1.50 mm
V-2
@Thickness 0.0591 in
IEC 60695-11-10
 V-2
@Thickness 0.800 mm
V-2
@Thickness 0.0315 in
IEC 60695-11-10
 
Descriptive Properties
AdditivesRelease agent
Delivery formPellets
Part Marking Code>PET-GF20FR<ISO 11469
ProcessingInjection Molding
Regional AvailabilityAsia Pacific
 Europe
 Global
 Near East/Africa
 North America
 South and Central America
UL recognitionUL

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Celanese Rynite® 408 NC010 PET
DuPont Mobility and Materials Rynite® FR530L NC010 Polyethylene Terephthalate (PET)
Idemitsu Kosan Xarec® EA 533 SPS, 30% Glass Filled
DuPont Mobility and Materials Rynite® FR530L BK507 Polyethylene Terephthalate (PET)
Celanese Rynite® RE15022 NC010 Polyethylene Terephthalate (PET)

PZDSY5283 / 161110

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.