MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

DuPont Mobility and Materials Rynite® FR530L NC010 Polyethylene Terephthalate (PET)  (discontinued **)
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), Glass Fiber Filled, Flame Retardant

Material Notes:

Rynite FR530 NC010 is a 30% glass reinforced flame retardant modified polyethylene terephthalate resin.

While this product line has been acquired by Celanese, this specific grade had been disconued while still a DuPont product so it is listed here as a discontinued DuPont product.

Key Words: PET-GF30FR(17)
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.68 g/cc0.0607 lb/in³ISO 1183
Water Absorption 0.75 %
@Thickness 2.00 mm
0.75 %
@Thickness 0.0787 in
Sim. to ISO 62
Moisture Absorption 0.150 %
@Thickness 2.00 mm
0.150 %
@Thickness 0.0787 in
Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0020 cm/cm0.0020 in/inISO 294-4 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cm0.0080 in/inISO 294-4 2577
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 280 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 536 °F
cm³/10min; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9595ASTM D785
Hardness, Rockwell R 120120ASTM D785
Tensile Strength at Break 135 MPa19600 psiISO 527-1/-2
Elongation at Break 2.0 %2.0 %ISO 527-1/-2
Tensile Modulus 11.5 GPa1670 ksiISO 527-1/-2
Flexural Modulus 10.5 GPa1520 ksiISO 178
Shear Modulus  0.525 GPa
@Temperature 160 °C
76.1 ksi
@Temperature 320 °F
Dynamic; ISO 11403-1 -2
 0.654 GPa
@Temperature 120 °C
94.9 ksi
@Temperature 248 °F
Dynamic; ISO 11403-1 -2
 1.151 GPa
@Temperature 70.0 °C
166.9 ksi
@Temperature 158 °F
Dynamic; ISO 11403-1 -2
 1.974 GPa
@Temperature 20.0 °C
286.3 ksi
@Temperature 68.0 °F
Dynamic; ISO 11403-1 -2
 2.208 GPa
@Temperature -20.0 °C
320.2 ksi
@Temperature -4.00 °F
Dynamic; ISO 11403-1 -2
 2.432 GPa
@Temperature -50.0 °C
352.7 ksi
@Temperature -58.0 °F
Dynamic; ISO 11403-1 -2
Charpy Impact Unnotched 4.00 J/cm²19.0 ft-lb/in²ISO 179/1eU
 4.00 J/cm²
@Temperature -30.0 °C
19.0 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
Charpy Impact, Notched 1.00 J/cm²4.76 ft-lb/in²ISO 179/1eA
 0.900 J/cm²
@Temperature -30.0 °C
4.28 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
Tensile Creep Modulus, 1 hour 11200 MPa
@Time 3600 sec
1.62e+6 psi
@Time 1.00 hour
ISO 899-1
Tensile Creep Modulus, 1000 hours 9700 MPa
@Time 3.60e+6 sec
1.41e+6 psi
@Time 1000 hour
ISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+15 ohm-cm1.00e+15 ohm-cmIEC 60093
Surface Resistance 1.00e+14 ohm1.00e+14 ohmIEC 60093
Dielectric Constant  3.7
@Frequency 1e+6 Hz
3.7
@Frequency 1e+6 Hz
ASTM D150
 3.8
@Frequency 1000 Hz
3.8
@Frequency 1000 Hz
ASTM D150
 4.7
@Frequency 1e+6 Hz
4.7
@Frequency 1e+6 Hz
IEC 60250
 4.8
@Frequency 100 Hz
4.8
@Frequency 100 Hz
IEC 60250
Dielectric Strength 33.0 kV/mm838 kV/inIEC 60243-1
Dissipation Factor  0.0070
@Frequency 100 Hz
0.0070
@Frequency 100 Hz
IEC 60250
 0.010
@Frequency 1e+6 Hz
0.010
@Frequency 1e+6 Hz
IEC 60250
 0.011
@Frequency 1000 Hz
0.011
@Frequency 1000 Hz
ASTM D150
 0.018
@Frequency 1e+6 Hz
0.018
@Frequency 1e+6 Hz
ASTM D150
Comparative Tracking Index 225 V225 VIEC 60112
 250 - 400 V250 - 400 VUL 746A
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 19.0 µm/m-°C10.6 µin/in-°FISO 11359-1/-2
 22.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
12.2 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 92.0 µm/m-°C51.1 µin/in-°FISO 11359-1/-2
 68.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
37.8 µin/in-°F
@Temperature -40.0 - 73.4 °F
ISO 11359-1/-2
Melting Point 252 °C486 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 243 °C469 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 225 °C437 °FISO 75-1/-2
Vicat Softening Point 220 °C428 °F50°C/h 50N; ISO 306
UL RTI, Electrical 155 °C
@Thickness 0.400 mm
311 °F
@Thickness 0.0157 in
UL 746B
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
IEC 60695-11-10
 V-0
@Thickness 0.300 mm
V-0
@Thickness 0.0118 in
IEC 60695-11-10
 5VA
@Thickness 0.900 mm
5VA
@Thickness 0.0354 in
IEC 60695-11-20
Oxygen Index 33 %33 %ISO 4589-1/-2
 33 %33 %ASTM D2863
 
Descriptive Properties
AdditivesRelease agent
Delivery formPellets
Part Marking Code>PET-GF30FR<ISO 11469
ProcessingInjection Molding
Regional AvailabilityEurope
 Near East/Africa
Resin IdentificationPET-GF30FR(17)
UL recognitionUL

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
DuPont Mobility and Materials Rynite® FR530L BK507 Polyethylene Terephthalate (PET)
Celanese Rynite® 408 NC010 PET
DuPont Mobility and Materials Rynite® GW520CS NC010 Polyethylene Terephthalate (PET)
Overview of materials for Polyethylene Terephthalate (PET), Unreinforced
Celanese Rynite® 530 NC010 PET-GF30

PZDSY5281 / 161108

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.