MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Titanium Ti-8Mn, Annealed
Categories: Metal; Nonferrous Metal; Titanium Alloy; Alpha/Beta Titanium Alloy

Material Notes: Annealed 705ºC. Alpha-Beta Alloy. Not weldable.

Applications: Aircraft, structural parts

Key Words: UNS R56080
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 4.73 g/cc0.171 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Brinell 318318Estimated from Rockwell C.
Hardness, Knoop 346346Estimated from Rockwell C.
Hardness, Rockwell C 3434
Hardness, Vickers 333333Estimated from Rockwell C.
Tensile Strength, Ultimate 900 MPa131000 psi
Tensile Strength, Yield 810 MPa117000 psi
Elongation at Break 14 %14 %
Reduction of Area 32 %32 %
Creep Strength  200 MPa
@Temperature 425 °C,
Time >=21600 sec
29000 psi
@Temperature 797 °F,
Time >=6.00 hour
strain 0.5%
 200 MPa
@Temperature 425 °C,
Time >=2880 sec
29000 psi
@Temperature 797 °F,
Time >=0.800 hour
strain 0.1%
 400 MPa
@Temperature 370 °C,
Time >=216000 sec
58000 psi
@Temperature 698 °F,
Time >=60.0 hour
strain 0.5%
 400 MPa
@Temperature 370 °C,
Time >=21600 sec
58000 psi
@Temperature 698 °F,
Time >=6.00 hour
strain 0.1%
Rupture Strength  >= 250 MPa
@Temperature 425 °C,
Time 360000 sec
>= 36300 psi
@Temperature 797 °F,
Time 100 hour
 600 MPa
@Temperature 370 °C,
Time 360000 sec
87000 psi
@Temperature 698 °F,
Time 100 hour
 >= 800 MPa
@Temperature 315 °C,
Time 360000 sec
>= 116000 psi
@Temperature 599 °F,
Time 100 hour
Modulus of Elasticity 115 GPa16700 ksiTypical value for annealed alpha/beta titanium alloy.
Modulus of Rigidity 48.3 GPa7010 ksi
Compressive Yield Strength 875 MPa127000 psi
Poissons Ratio 0.330.33Typical for alpha-beta titanium alloy.
Fatigue Strength  210 MPa
@# of Cycles 1.00e+7
30500 psi
@# of Cycles 1.00e+7
Rotating Beam. Kt (stress concentration factor) = 3.0
 400 MPa
@# of Cycles 10000
58000 psi
@# of Cycles 10000
Rotating Beam. Kt (stress concentration factor) = 3.0
 585 MPa
@# of Cycles 1.00e+7
84800 psi
@# of Cycles 1.00e+7
Unnotched Sheet
 800 MPa
@# of Cycles 2000
116000 psi
@# of Cycles 2000
unnotched
Shear Modulus 43.2 GPa6270 ksiCalculated from typical values.
Bend Radius, Minimum 3.0 t3.0 t
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000920 ohm-cm0.0000920 ohm-cm
Magnetic Permeability 1.000051.00005at 1.6 kA/m
 
Thermal PropertiesMetricEnglishComments
CTE, linear  8.60 µm/m-°C
@Temperature 20.0 - 100 °C
4.78 µin/in-°F
@Temperature 68.0 - 212 °F
 9.70 µm/m-°C
@Temperature 20.0 - 315 °C
5.39 µin/in-°F
@Temperature 68.0 - 599 °F
average
 11.7 µm/m-°C
@Temperature 20.0 - 650 °C
6.50 µin/in-°F
@Temperature 68.0 - 1200 °F
average
Specific Heat Capacity 0.495 J/g-°C0.118 BTU/lb-°F
Thermal Conductivity  10.9 W/m-K
@Temperature 20.0 °C
75.6 BTU-in/hr-ft²-°F
@Temperature 68.0 °F
 12.8 W/m-K
@Temperature 205 °C
88.8 BTU-in/hr-ft²-°F
@Temperature 401 °F
 15.2 W/m-K
@Temperature 425 °C
105 BTU-in/hr-ft²-°F
@Temperature 797 °F
 17.8 W/m-K
@Temperature 650 °C
124 BTU-in/hr-ft²-°F
@Temperature 1200 °F
Melting Point 1565 °C2849 °F
Solidus 1300 °C2370 °F
Liquidus 1635 °C2975 °F
Beta Transus 785 - 815 °C1450 - 1500 °F
 
Component Elements PropertiesMetricEnglishComments
Carbon, C <= 0.20 %<= 0.20 %
Hydrogen, H <= 0.015 %<= 0.015 %
Manganese, Mn 8.0 %8.0 %
Nitrogen, N <= 0.070 %<= 0.070 %
Oxygen, O <= 0.20 %<= 0.20 %
Titanium, Ti 92 %92 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum 2024-T3
Medical Grade Stainless Steel 316LVM
Sandvik Bioline 316LVM Tube and pipe, seamless
Overview of materials for Alpha/Beta Titanium Alloy
Ti6Al7Nb ASTM F1295

MTP081 / 14226

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.