MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Celanese Rynite® 530 BK503 PET-GF30
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 30% Glass Reinforced

Material Notes: 30% Glass Reinforced Polyethylene Terephthalate

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.56 g/cc0.0564 lb/in³ISO 1183
Water Absorption 0.050 %
@Time 86400 sec
0.050 %
@Time 24.0 hour
Immersion; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cm0.0030 in/inISO 294-4, 2577
 0.0010 cm/cm
@Treatment Temp. 80.0 °C,
Time 173000 sec
0.0010 in/in
@Treatment Temp. 176 °F,
Time 48.0 hour
Postmolding shrinkage; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cm0.0090 in/inISO 294-4, 2577
 0.0045 cm/cm
@Treatment Temp. 80.0 °C,
Time 173000 sec
0.0045 in/in
@Treatment Temp. 176 °F,
Time 48.0 hour
Postmolding shrinkage; ISO 294-4
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell R 120120ISO 2039-2
Ball Indentation Hardness 221 MPa32100 psiH 961/30; ISO 2039-1
Tensile Strength at Break 150 MPa21800 psiISO 527-1/-2
Elongation at Break 2.1 %2.1 %ISO 527-1/-2
Tensile Modulus 10.2 GPa1480 ksiISO 527-1/-2
Flexural Strength 210 MPa30500 psiISO 178
Flexural Modulus 8.94 GPa1300 ksiISO 178
Compressive Strength 230 MPa33400 psiISO 604
Poissons Ratio 0.340.34
Izod Impact, Notched (ISO)  8.50 kJ/m²
@Temperature -40.0 °C
4.04 ft-lb/in²
@Temperature -40.0 °F
ISO 180/1A
 9.50 kJ/m²
@Temperature 23.0 °C
4.52 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1A
Izod Impact, Unnotched (ISO)  35.0 kJ/m²
@Temperature -40.0 °C
16.7 ft-lb/in²
@Temperature -40.0 °F
ISO 180/1U
 45.0 kJ/m²
@Temperature 23.0 °C
21.4 ft-lb/in²
@Temperature 73.4 °F
ISO 180/1U
Charpy Impact Unnotched  4.50 J/cm²
@Temperature -40.0 °C
21.4 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eU
 5.20 J/cm²
@Temperature 23.0 °C
24.7 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  0.800 J/cm²
@Temperature -40.0 °C
3.81 ft-lb/in²
@Temperature -40.0 °F
ISO 179/1eA
 0.850 J/cm²
@Temperature -30.0 °C
4.04 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 0.950 J/cm²
@Temperature 23.0 °C
4.52 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Surface Resistance >= 1.00e+15 ohm>= 1.00e+15 ohmIEC 62631-3-2
Dielectric Constant  4.2
@Frequency 1e+6 Hz
4.2
@Frequency 1e+6 Hz
IEC 62631-2-1
 4.5
@Frequency 100 Hz
4.5
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 32.0 kV/mm813 kV/inIEC 60243-1
Dissipation Factor  0.0152
@Frequency 1e+6 Hz
0.0152
@Frequency 1e+6 Hz
IEC 62631-2-1
 0.031
@Frequency 100 Hz
0.031
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 250 V250 VIEC 60112
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.290 W/m-K2.01 BTU-in/hr-ft²-°FSolid
Melting Point 250 °C482 °F10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 244 °C471 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 221 °C430 °FISO 75-1/-2
Glass Transition Temp, Tg 90.0 °C194 °F10°C/min; ISO 11357-1/-2
Flammability, UL94  HB
@Thickness 0.810 mm
HB
@Thickness 0.0319 in
IEC 60695-11-10
 HB
@Thickness 1.50 mm
HB
@Thickness 0.0591 in
IEC 60695-11-10
Flame Spread 38.0 mm/min
@Thickness 1.00 mm
1.50 in/min
@Thickness 0.0394 in
ISO 3795 (FMVSS 302)
 
Processing PropertiesMetricEnglishComments
Melt Temperature 285 °C545 °FOptimum, Injection
 280 - 300 °C536 - 572 °FRange, Injection
Mold Temperature 120 °C248 °FOptimum, Injection
 110 - 130 °C230 - 266 °FInjection
Ejection Temperature 170 °C338 °FInjection
Drying Temperature 120 °C248 °FInjection
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.020 %<= 0.020 %Injection
Hold Pressure >= 80.0 MPa>= 11600 psiInjection
 
Descriptive Properties
Back pressureAs low as possible
Drying RecommendedyesInjection
Emission of organic compounds (µgC/g)16VDA 277
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging (mg)0G-value (condensate); ISO 6452
Max. screw tangential speed (m/s)0.2Injection
Odor Class3VDA 270
Part Marking Code>PET-GF30<ISO 11469
PolymerPET-GF30
Processing Hold Pressure Time (s/mm)4Injection
Resin IdentificationPET-GF30ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® Rx1805 Polycarbonate
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Celanese Rynite® 530 NC010 PET-GF30
Covestro Makrolon® 9417 Polycarbonate, 10% Glass Filled
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant

PDSX5258 / 197898

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.