MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makrolon® 9417 Polycarbonate, 10% Glass Filled
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, 10% Glass Filled

Material Notes: MVR (300 °C/1.2 kg) 6.0 cm³/10 min; 10 % glass fiber reinforced; flame retardant; UL 94V-0/1.5 mm and 5VA/3.0 mm; high viscosity; UV stabilized; easy release; injection molding - melt temperature 310 - 330 °C; available in opaque colors only

As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and officially adopted its new name – Covestro.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.640 g/cc0.0231 lb/in³Pellets; ISO 60
Density 1.27 g/cc0.0459 lb/in³ISO 1183
Water Absorption 0.26 %0.26 %ISO 62
Moisture Absorption at Equilibrium 0.10 %0.10 %ISO 62
Linear Mold Shrinkage 0.0040 - 0.0060 cm/cm0.0040 - 0.0060 in/inparallel/normal; b.o. ISO 2577
Linear Mold Shrinkage, Flow 0.0060 cm/cm0.0060 in/in60x60x2 mm; 500 bar; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0045 cm/cm0.0045 in/in60x60x2 mm; 500 bar; ISO 294-4
Melt Flow 7.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
7.0 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 128 MPa18600 psiISO 2039-1
Tensile Strength at Break 45.0 MPa6530 psi50 mm/min; ISO 527-1/-2
Tensile Strength, Yield 64.0 MPa9280 psi50 mm/min; ISO 527-1/-2
Elongation at Break 15 %15 %50 mm/min; ISO 527-1/-2
Elongation at Yield 4.6 %4.6 %50 mm/min; ISO 527-1/-2
Tensile Modulus 3.80 GPa551 ksi1 mm/min; ISO 527-1/-2
Flexural Strength 105 MPa15200 psi2 mm/min; ISO 178
Flexural Yield Strength 95.0 MPa
@Strain 3.5 %
13800 psi
@Strain 3.5 %
2 mm/min; ISO 178
Flexural Modulus 3.60 GPa522 ksi2 mm/min; ISO 178
Flexural Strain at Yield 5.8 %5.8 %2 mm/min; ISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Thickness 23.0 mm
4.76 ft-lb/in²
@Thickness 0.906 in
complete break; ISO 7391/b.o. ISO 180-A
Charpy Impact Unnotched  10.0 J/cm²
@Temperature -60.0 °C
47.6 ft-lb/in²
@Temperature -76.0 °F
complete break; ISO 179-1eU
 12.0 J/cm²
@Temperature -30.0 °C
57.1 ft-lb/in²
@Temperature -22.0 °F
complete break; ISO 179-1eU
 15.0 J/cm²
@Temperature 23.0 °C
71.4 ft-lb/in²
@Temperature 73.4 °F
complete break; ISO 179-1eU
Charpy Impact, Notched 1.00 J/cm²
@Thickness 23.0 mm
4.76 ft-lb/in²
@Thickness 0.906 in
complete break; ISO 7391/b.o. ISO 179-1eA
Impact 40004000Puncture - maximum force (N); ISO 6603-2
 3700
@Temperature -30.0 °C
3700
@Temperature -22.0 °F
Puncture - maximum force (N); ISO 6603-2
Puncture Energy 25.0 J18.4 ft-lbISO 6603-2
 15.0 J
@Temperature -30.0 °C
11.1 ft-lb
@Temperature -22.0 °F
ISO 6603-2
Tensile Creep Modulus, 1 hour 3600 MPa522000 psiISO 899-1
Tensile Creep Modulus, 1000 hours 2900 MPa421000 psiISO 899-1
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmIEC 60093
Surface Resistance 1.00e+16 ohm1.00e+16 ohmIEC 60093
Dielectric Constant  3.2
@Frequency 100 Hz
3.2
@Frequency 100 Hz
IEC 60250
 3.2
@Frequency 1e+6 Hz
3.2
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 36.0 kV/mm914 kV/in1 mm; IEC 60243-1
Dissipation Factor  0.0010
@Frequency 100 Hz
0.0010
@Frequency 100 Hz
IEC 60250
 0.0090
@Frequency 1e+6 Hz
0.0090
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 125 V125 VCTI M; Solution B; IEC 60112
 175 V175 VSolution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 40.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
22.2 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
CTE, linear, Transverse to Flow 65.0 µm/m-°C
@Temperature 23.0 - 55.0 °C
36.1 µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1/-2
Specific Heat Capacity 1.60 J/g-°C0.382 BTU/lb-°FMelt
Thermal Conductivity 0.220 W/m-K1.53 BTU-in/hr-ft²-°Fcross-flow; ISO 8302
Hot Ball Pressure Test 136 °C277 °FIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 141 °C286 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 135 °C275 °FISO 75-1/-2
Vicat Softening Point 143 °C289 °F50°C/h 50N; ISO 306
 144 °C291 °F50 N; 120 °C/h; ISO 306
UL RTI, Electrical 125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
UL 746B
UL RTI, Mechanical with Impact 115 °C
@Thickness 1.50 mm
239 °F
@Thickness 0.0591 in
UL 746B
UL RTI, Mechanical without Impact 125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
UL 746B
Flammability, UL94  V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
IEC 60695-11-10
 5VA
@Thickness 6.00 mm
5VA
@Thickness 0.236 in
IEC 60695-11-10
 5VA
@Thickness 3.00 mm
5VA
@Thickness 0.118 in
IEC 60695-11-20
Flash Point 470 °C878 °Fignition; ASTM D1929
 550 °C1020 °Fself ignition; ASTM D1929
Oxygen Index 35 %35 %Method A; ISO 4589-1/-2
Glow Wire Ignition Temperature  825 °C
@Thickness 1.00 mm
1520 °F
@Thickness 0.0394 in
IEC 60695-2-13
 900 °C
@Thickness 1.50 mm
1650 °F
@Thickness 0.0591 in
IEC 60695-2-13
 900 °C
@Thickness 3.00 mm
1650 °F
@Thickness 0.118 in
IEC 60695-2-13
Glow Wire Flammability Index  960 °C
@Thickness 0.750 mm
1760 °F
@Thickness 0.0295 in
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
1760 °F
@Thickness 0.0591 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Processing PropertiesMetricEnglishComments
Melt Temperature 300 °C572 °FInjection Molding; ISO 294
Mold Temperature 110 °C230 °FInjection Molding; ISO 294
Ejection Temperature 140 °C284 °F
 
Descriptive Properties
Electrolytic corrosionA1IEC 60426

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® Rx1805 Polycarbonate
Covestro Makrolon® 2865 Polycarbonate, Flame Retardant Grade
Celanese Rynite® 530 BK503 PET-GF30
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant
Covestro Makrolon® 9415 Polycarbonate, 10% Glass Filled

PB09944 / 92784

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.