MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® 8552 Epoxy Matrix, AS4 Fiber
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes:

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  75.2 MPa
@Temperature 93.3 °C
10900 psi
@Temperature 200 °F
90°, Dry
 80.7 MPa
@Temperature 25.0 °C
11700 psi
@Temperature 77.0 °F
90°, Dry
 438 MPa
@Temperature 25.0 °C
63500 psi
@Temperature 77.0 °F
Open Hole Tensile, Dry
 738 MPa
@Temperature 25.0 °C
107000 psi
@Temperature 77.0 °F
Quasi-Isotropic 25/50/25, Dry
 1900 MPa
@Temperature -55.0 °C
276000 psi
@Temperature -67.0 °F
0°, Dry
 2020 MPa
@Temperature 90.6 °C
293000 psi
@Temperature 195 °F
0°, Dry
 2140 MPa
@Temperature 25.0 °C
310000 psi
@Temperature 77.0 °F
0°, Dry
Tensile Modulus  8.41 GPa
@Temperature 200 °C
1220 ksi
@Temperature 392 °F
90°, Dry
 9.58 GPa
@Temperature 77.0 °C
1390 ksi
@Temperature 171 °F
90°, Dry
 132 GPa
@Temperature 195 °C
19100 ksi
@Temperature 383 °F
0°, Dry
 134 GPa
@Temperature -67.0 °C
19400 ksi
@Temperature -88.6 °F
0°, Dry
 135 GPa
@Temperature 77.0 °C
19600 ksi
@Temperature 171 °F
0°, Dry
Flexural Yield Strength 1890 MPa
@Temperature 25.0 °C
274000 psi
@Temperature 77.0 °F
0°, Dry
Flexural Modulus 127 GPa
@Temperature 25.0 °C
18400 ksi
@Temperature 77.0 °F
0°, Dry
Compressive Yield Strength  186 MPa
@Temperature 25.0 °C
27000 psi
@Temperature 77.0 °F
After 2500 in-in-lb/in impact, Dry
 193 MPa
@Temperature 25.0 °C
28000 psi
@Temperature 77.0 °F
After 2000 in-in-lb/in impact, Dry
 221 MPa
@Temperature 25.0 °C
32000 psi
@Temperature 77.0 °F
After 1500 in-in-lb/in impact, Dry
 239 MPa
@Temperature 25.0 °C
34600 psi
@Temperature 77.0 °F
Compression After Impact, Dry
 345 MPa
@Temperature 25.0 °C
50000 psi
@Temperature 77.0 °F
After 500 in-in-lb/in impact, Dry
 629 MPa
@Temperature 25.0 °C
91200 psi
@Temperature 77.0 °F
Compression Before Impact, Dry
 1270 MPa
@Temperature 90.6 °C
184000 psi
@Temperature 195 °F
0°, Dry
 1270 MPa
@Temperature 90.6 °C
184000 psi
@Temperature 195 °F
0°, Wet
 1400 MPa
@Temperature 71.1 °C
203000 psi
@Temperature 160 °F
0°, Wet
 1530 MPa
@Temperature 25.0 °C
222000 psi
@Temperature 77.0 °F
0°, Dry
 1590 MPa
@Temperature -55.0 °C
230000 psi
@Temperature -67.0 °F
0°, Dry
Compressive Modulus  117 GPa
@Temperature 71.1 °C
17000 ksi
@Temperature 160 °F
0°, Wet
 122 GPa
@Temperature 90.6 °C
17700 ksi
@Temperature 195 °F
0°, Dry
 124 GPa
@Temperature -55.0 °C
18000 ksi
@Temperature -67.0 °F
0°, Dry
 125 GPa
@Temperature 90.6 °C
18100 ksi
@Temperature 195 °F
0°, Wet
 128 GPa
@Temperature 25.0 °C
18600 ksi
@Temperature 77.0 °F
0°, Dry
Shear Strength  77.9 MPa
@Temperature 90.6 °C
11300 psi
@Temperature 195 °F
0° Short Beam, Wet
 84.1 MPa
@Temperature 71.1 °C
12200 psi
@Temperature 160 °F
0° Short Beam, Wet
 101 MPa
@Temperature 90.6 °C
14700 psi
@Temperature 195 °F
0° Short Beam, Dry
 105 MPa
@Temperature 93.3 °C
15200 psi
@Temperature 200 °F
+/- 45° In-Plane, Dry
 114 MPa
@Temperature 25.0 °C
16600 psi
@Temperature 77.0 °F
+/- 45° In-Plane, Dry
 117 MPa
@Temperature 25.0 °C
16900 psi
@Temperature 77.0 °F
0° Short Beam, Wet
 128 MPa
@Temperature 25.0 °C
18500 psi
@Temperature 77.0 °F
0° Short Beam, Dry
 164 MPa
@Temperature -55.0 °C
23800 psi
@Temperature -67.0 °F
0° Short Beam, Dry
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 121 °C250 °FEpoxy Matrix Limit

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® 8552 Epoxy Matrix
Hexcel® HexPly® 8552 Epoxy Matrix, IM7 Fiber
Hexcel® HexTow® IM7 6K Intermediate Modulus Carbon Fiber (6000 Filaments)
Hexcel® HexTow® IM7 Carbon Fiber - Epoxy Composite
Hexcel® HexPly® 8551-7 Epoxy Matrix, AS4 Fiber

PHEXC052 / 98522

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.