MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BCC Products BC 6004 Epoxy Surface Coat
Categories: Polymer; Thermoset; Epoxy

Material Notes: BC 6004 is a white thixotropic epoxy surface coat that has the ability to cure and bond to freshly poured wet plaster. This formulated resin compound can be applied with a brush or troweled to a thickness of 1/8” or less on vertical surfaces or over sharp radii without sag or fear of run-off. BC 6004 features moderate heat resistance and tracing hardness.

Information provided by BCC Products, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.58 g/cc1.58 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 89
@Temperature 23.9 °C
89
@Temperature 75.0 °F
Tensile Strength, Ultimate 46.9 MPa6800 psi
Flexural Strength 59.3 MPa8600 psi
Flexural Modulus 6.76 GPa980 ksi
Compressive Strength 95.1 MPa13800 psi
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 1.8 MPa (264 psi) 78.9 °C174 °F
 
Processing PropertiesMetricEnglishComments
Cure Time 480 - 720 min
@Temperature 24.0 °C
8.00 - 12.0 hour
@Temperature 75.2 °F
Pot Life 15 - 20 min
@Temperature 24.0 °C
15 - 20 min
@Temperature 75.2 °F
4 oz. mass
 
Descriptive Properties
Mix Ratio12:1 by weight, 7:1 by volume, resin/harder
Mixed Viscosity, BrookfieldThixotropic

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aremco Aremco-Bond™ 2335 Ultra High Temperature Epoxy
Bakelite® EP 8412 Epoxy Resin, High Arc Resistance, Improved Electrical Properties, Low Shrinkage
Overview of materials for Epoxy, Cycloaliphatic, Molded
Arlon Electronic Materials 45N Multifunctional Epoxy Laminate and Prepreg
Atom Adhesives AA-BOND F110 Epoxy Adhesive

PBCC026 / 107253

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.