MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil Optema® TC-110 Blown Ethylene Methyl Acrylate
Categories: Polymer; Film; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Extrusion Grade

Material Notes: Product Description: Optema TC 110 is an ethylene methyl acrylate copolymer specifically formulated to offer extrusion and property performance for blown film applications. It produces a soft, elastic film with good handling characteristics without additional additives. It can produce film under 1.0 mil thickness.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Disposable Gloves
  • Hospital Drapes
  • Upholstery Film

Data provided by the manufacturer, Exxon Chemical.

Key Words: EMA; Exxon Chemical Company
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.942 g/cc0.0340 lb/in³Exxon Method
Methyl Acrylate Content 21.5 %21.5 %Exxon Method
Thickness 31.8 microns1.25 mil
Melt Flow 2.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
2.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Elongation at Break, MD 370 %370 %ASTM D882
Film Elongation at Break, TD 650 %650 %ASTM D882
Elmendorf Tear Strength MD 30 g30 gASTM D1922
Elmendorf Tear Strength TD 320 g320 gASTM D1922
Dart Drop Test 430 g0.948 lbASTM D1709A
Film Tensile Strength at Break, MD 20.0 MPa2900 psiASTM D882
Film Tensile Strength at Break, TD 20.7 MPa3000 psiASTM D882
1% Secant Modulus, MD 42.7 MPa6200 psiASTM D882
1% Secant Modulus, TD 40.0 MPa5800 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 176 °C349 °FPeak Temperature; Exxon Method
Vicat Softening Point 127 °C261 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 16 %16 %ASTM D1003
Gloss 34 %34 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil Optema® TC-110 Cast Ethylene Methyl Acrylate
ExxonMobil Optema® TC-110 Molding Ethylene Methyl Acrylate
ExxonMobil Optema® TC-114 Blown Ethylene Methyl Acrylate
ExxonMobil Optema® TC-114 Cast Ethylene Methyl Acrylate
ExxonMobil OPTEMA™ TC 120 ExCo Ethylene Methyl Acrylate

PEXCEU / 37906

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.