MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

ExxonMobil OPTEMA™ TC 120 ExCo Ethylene Methyl Acrylate
Categories: Polymer; Thermoplastic; Ethylene Methyl Acrylate; Ethylene-Methyl Acrylate Copolymer, Molding Grade

Material Notes: Product Description: Optema TC 120 is an ethylene methyl acrylate copolymer intended for extrusion coating, coextrusion coating and extrusion lamination where good interlayer adhesion between polyethylene, polypropylene, nylon, PVdC or other substrates is required. It offers excellent balance of adhesion onto the substrates and interlayer adhesion with coextruded LDPE and EVA’s. It is an excellent heat seal layer in coextrusion and in extrusion coating but additional additives or process modifications may be required to prevent chill roll sticking.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Coextrustion Coating
  • Demanding Heat Seals
  • Document Plastification
  • Extrusion Coating
  • Extrusion Lamination
  • Food packaging
  • Industrial Packaging
  • Non-Woven Coating
  • Thermal Lamination
Information provided by ExxonMobil Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.942 g/cc0.0340 lb/in³ExxonMobil Method
Methyl Acrylate Content 21.5 %21.5 %
Melt Flow 6.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
6.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Neck In  5.59 cm
@Temperature 295 °C
2.20 in
@Temperature 563 °F
656 ft/min, Constant output at 35 rpm; ExxonMobil Method
 6.10 cm
@Temperature 295 °C
2.40 in
@Temperature 563 °F
328 ft/min, Constant output at 35 rpm; ExxonMobil Method
Drawdown 6.60 m/s
@Temperature 295 °C
1300 ft/min
@Temperature 563 °F
Constant output at 35 rpm; ExxonMobil Method
 
Thermal PropertiesMetricEnglishComments
Melting Point 77.8 °C172 °FPeak Melting Temperature; ExxonMobil Method
Vicat Softening Point 47.2 °C117 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil OPTEMA™ TC 220 ExCo Ethylene Methyl Acrylate
DuPont Elvaloy® 1126 AC Ethylene and 25% Methyl Acrylate Copolymer
ExxonMobil Optema® TC-110 Blown Ethylene Methyl Acrylate
ExxonMobil Optema® TC-110 Cast Ethylene Methyl Acrylate
ExxonMobil Optema® TC-110 Molding Ethylene Methyl Acrylate

PEXB172a / 141037

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.