Physical Properties | Metric | English | Comments |
---|
Specific Gravity | 2.12 - 2.17 g/cc | 2.12 - 2.17 g/cc |
Water Absorption | <= 0.030 % | <= 0.030 % |
Melt Flow | 14 g/10 min | 14 g/10 min |
|
Mechanical Properties | Metric | English | Comments |
---|
Hardness, Shore D | 55 | 55 |
Tensile Strength, Ultimate | 25.0 MPa | 3630 psi |
| 12.0 MPa @Temperature 250 °C | 1740 psi @Temperature 482 °F |
| 129 MPa @Temperature -196 °C | 18700 psi @Temperature -321 °F |
Tensile Strength, Yield | 13.8 MPa | 2000 psi |
Elongation at Break | 300 % | 300 % |
| 8.0 % @Temperature -196 °C | 8.0 % @Temperature -321 °F |
| 480 % @Temperature 250 °C | 480 % @Temperature 482 °F |
Flexural Modulus | 0.590 GPa | 85.6 ksi |
| 0.0550 GPa @Temperature 250 °C | 7.98 ksi @Temperature 482 °F |
Compressive Strength | 24.0 MPa @Temperature 23.0 °C | 3480 psi @Temperature 73.4 °F |
| 414 MPa @Temperature -196 °C | 60000 psi @Temperature -321 °F |
Compressive Modulus | 69.0 GPa @Temperature 23.0 °C | 10000 ksi @Temperature 73.4 °F |
| 4690 GPa @Temperature -196 °C | 680000 ksi @Temperature -321 °F |
Izod Impact, Notched | NB | NB |
| 0.640 J/cm @Temperature -196 °C | 1.20 ft-lb/in @Temperature -321 °F |
Coefficient of Friction, Dynamic | 0.21 | 0.21 |
| 0.214 | 0.214 |
| 0.229 | 0.229 |
| 0.289 | 0.289 |
K (wear) Factor | 1400 x 10-8 mm³/N-M | 694 x 10-10 in³-min/ft-lb-hr |
| 1980 x 10-8 mm³/N-M | 983 x 10-10 in³-min/ft-lb-hr |
| 3205 x 10-8 mm³/N-M | 1591 x 10-10 in³-min/ft-lb-hr |
| 3700 x 10-8 mm³/N-M | 1837 x 10-10 in³-min/ft-lb-hr |
|
Electrical Properties | Metric | English | Comments |
---|
Volume Resistivity | 1.00e+18 ohm-cm | 1.00e+18 ohm-cm |
Surface Resistivity per Square | >= 1.00e+17 ohm | >= 1.00e+17 ohm |
Dielectric Constant | 2.03 @Frequency 60.0 - 1.00e+6 Hz | 2.03 @Frequency 60.0 - 1.00e+6 Hz |
Dielectric Strength | 80.0 kV/mm @Thickness 0.0250 mm | 2030 kV/in @Thickness 0.000984 in |
Dissipation Factor | 0.00010 @Frequency 60.0 - 1.00e+6 Hz | 0.00010 @Frequency 60.0 - 1.00e+6 Hz |
Arc Resistance | >= 180 sec | >= 180 sec |
|
Thermal Properties | Metric | English | Comments |
---|
CTE, linear | 140 µm/m-°C @Temperature 21.0 - 100 °C | 77.8 µin/in-°F @Temperature 69.8 - 212 °F |
| 170 µm/m-°C @Temperature 100 - 149 °C | 94.4 µin/in-°F @Temperature 212 - 300 °F |
| 210 µm/m-°C @Temperature 149 - 208 °C | 117 µin/in-°F @Temperature 300 - 406 °F |
Specific Heat Capacity | 1.172 J/g-°C @Temperature 100 °C | 0.2801 BTU/lb-°F @Temperature 212 °F |
Melting Point | 302 - 310 °C | 576 - 590 °F |
Maximum Service Temperature, Air | 260 °C | 500 °F |
Glass Transition Temp, Tg | -80.0 °C | -112 °F |
| 90.0 °C | 194 °F |
Flammability, UL94 | V-0 | V-0 |
Oxygen Index | >= 95 % | >= 95 % |
|
Optical Properties | Metric | English | Comments |
---|
Refractive Index | 1.35 | 1.35 |
Haze | 4.0 % | 4.0 % |
Transmission, Visible | 91 - 96 % @Thickness 0.0250 mm | 91 - 96 % @Thickness 0.000984 in |
IR Transmittance | 96 - 98 % | 96 - 98 % |
UV Transmittance | 77 - 91 % @Thickness 0.0250 mm | 77 - 91 % @Thickness 0.000984 in |
|
Processing Properties | Metric | English | Comments |
---|
Processing Temperature | 379 - 399 °C | 714 - 750 °F |
|
Descriptive Properties |
---|
20% Hydrochloric Acid Transmission, g/100sq in. | <0.02 |
50% Sodium Hydroxide Transmission, g/100sq in. | <.02 |
Acetic Acid Transmission, g/100sq in. | 0.41 |
Acetone Transmission, g/100sq in. | 0.95 |
Acetophenone Transmission, g/100sq in. | 0.5 |
Benzene Transmission, g/100sq in. | 0.64 |
Carbon Tetrachloride Transmission, g/100sq in. | 0.31 |
Chemical/Solvent Resistance | Excellent |
Ethyl Acetate Transmission, g/100sq in. | 0.76 |
Folding Endurance, # cycles, .18-.20 mm | 15000 |
Heat of Combustion J/g | 5300 |
Hexane Transmission, g/100sq in. | 0.56 |
Piperidine Transmission, g/100sq in. | 0.04 |
Red Fuming Nitric Acid Transmission, g/100sq in. | 7.5-1.4 |
Salt Spray Resistance on aluminum, Hours | 1000 |
Sulfuric Acid Transmission, g/100sq in. | 0.00001 |
Water Transmission, g/100sq in. | 0.4 |
Weather Resistance | 10 |
Some of the values displayed above may have been converted from their original units and/or rounded in order to
display the information in a consistent format. Users requiring more precise data for scientific or engineering
calculations can click on the property value to see the original value as well as raw conversions to equivalent units.
We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding
error. We also ask that you refer to MatWeb's
terms of use regarding this information.
Click here to view
all the property values for this datasheet as they were originally entered into MatWeb.