MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Versalis Flexirene® FG 30 Butene Copolymer Linear Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Butene, Film

Material Notes: Flexirene FG 30 is a butene copolymer linear low density polyethylene (C4-LLDPE), with antioxidants, suitable for blown film extrusion.

Films manufactured with Flexirene FG 30 are characterized by an optimum balance between mechanical properties (stiffness) and sealing properties.

Main Applications: Flexirene FG 30 is recommended for the production of general purpose film, automatic packaging and food packaging, especially when food is submitted to continuous cooking.

Information provided by Polimeri Europa.

Versalis is the Eni subsidiary containing the plastics and rubber businesses.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.925 g/cc0.925 g/ccISO 1183
Thickness 15.0 - 50.0 microns0.591 - 1.97 milRecommended
Melt Flow 1.0 g/10 min
@Load 2.16 kg,
Temperature 190 °C
1.0 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 12.0 MPa1740 psiISO 527-3
Film Tensile Strength at Yield, TD 13.0 MPa1890 psiISO 527-3
Film Elongation at Break, MD 600 %600 %ISO 527-3
Film Elongation at Break, TD 800 %800 %ISO 527-3
Coefficient of Friction, Dynamic >= 0.50>= 0.50ISO 8295
Elmendorf Tear Strength, MD 2.5475 g/micron64.706 g/milISO 6383-2
Elmendorf Tear Strength, TD 18.342 g/micron465.89 g/milISO 6383-2
Dart Drop Test 60.0 g0.132 lbF50; ISO 7765-1
Film Tensile Strength at Break, MD 45.0 MPa6530 psiISO 527-3
Film Tensile Strength at Break, TD 33.0 MPa4790 psiISO 527-3
1% Secant Modulus, MD 250 MPa36300 psiISO 527-3
1% Secant Modulus, TD 290 MPa42100 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 124 °C255 °FInternal method
Vicat Softening Point 105 °C
@Load 1.00 kg
221 °F
@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C<= -94.0 °FASTM D746
 
Optical PropertiesMetricEnglishComments
Haze 13 %13 %ISO 14782
Gloss 50 %50 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
ExxonMobil LD 07523.BW Low Density Polyethylene Resin
ExxonMobil LD 07523.AC Low Density Polyethylene Resin
ExxonMobil HD 6207 High Density Polyethylene Resin
ExxonMobil HD 5404 High Density Polyethylene Resin
ExxonMobil LDPE LD 380BA Blown Low Density Polyethylene Resin (European Grade)

PENG094 / 124488

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.