System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
Categories:
Polymer
;
Adhesive
;
Thermoset
;
Epoxy
;
Epoxy Adhesive
Material Notes:
3M™ Scotch-Weld™ Epoxy Adhesive DP460 Off-White and DP460 NS are high performance, two-part epoxy adhesives offering outstanding shear and peel adhesion and very high levels of durability.
Information provided by 3M
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Viscosity
8000
-
14000
cP
8000
-
14000
cP
Accelerator
150000
-
275000
cP
150000
-
275000
cP
Base
Mechanical Properties
Metric
English
Comments
Hardness, Shore D
78 - 84
78 - 84
Shear Strength
0.621
MPa
90.0
psi
Overlap, Isopropyl Alcohol Wipe surface prep, Neoprene/Steel
0.786
MPa
114
psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Neoprene/Steel
0.896
MPa
130
psi
Overlap, Isopropyl Alcohol Wipe surface prep, SBR/Steel
1.45
MPa
210
psi
Overlap, Isopropyl Alcohol Wipe surface prep, Polyacrylic
1.65
MPa
239
psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, SBR/Steel
1.86
MPa
270
psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polyacrylic
2.16
MPa
313
psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, PVC
2.21
MPa
320
psi
Overlap, Isopropyl Alcohol Wipe surface prep, Polystyrene
2.38
MPa
345
psi
Overlap, Isopropyl Alcohol Wipe surface prep, ABS
2.62
MPa
380
psi
Overlap, Isopropyl Alcohol Wipe surface prep, Polycarbonate
2.69
MPa
390
psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polycarbonate
3.38
MPa
490
psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Polystyrene
3.93
MPa
570
psi
Overlap, Isopropyl Alcohol Wipe surface prep, FRP
3.94
MPa
572
psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, ABS
5.62
MPa
815
psi
Overlap, Isopropyl Alcohol Wipe surface prep, PVC
8.34
MPa
1210
psi
Overlap, Isopropyl Alcohol Wipe surface prep, Phenolic
8.487
MPa
1231
psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol surface prep, Phenolic
9.508
MPa
1379
psi
Overlap, Isopropyl Alcohol/Abrade/Isopropyl Alcohol Wipe surface prep, FRP
15.9
MPa
2300
psi
Overlap, Aluminum Oakite degrease
16.5
MPa
2400
psi
Overlap, Stainless Steel MEK/abrade/MEK
17.1
MPa
2480
psi
Overlap, Galvanized Steel Okite degrease Hot dip
18.4
MPa
2670
psi
Overlap, Aluminum MEK/abrade/MEK
20.7
MPa
3000
psi
Overlap, Galvanized Steel Okite degrease Electrodeposited
23.4
MPa
3400
psi
Overlap, Brass MEK/abrade/MEK
24.8
MPa
3600
psi
Overlap, CRS MEK/abrade/MEK
30.3
MPa
4400
psi
Overlap, Copper MEK/abrade/MEK
31.0
MPa
4500
psi
Overlap, Aluminum Etched
32.1
MPa
@Temperature 23.0 °C
4650
psi
@Temperature 73.4 °F
Aluminum, Overlap
33.8
MPa
@Temperature -55.0 °C
4900
psi
@Temperature -67.0 °F
Aluminum, Overlap
2.90
MPa
@Temperature 121 °C,
Time 900 sec
420
psi
@Temperature 250 °F,
Time 0.250 hour
Aluminum, Overlap
9.38
MPa
@Temperature 82.0 °C,
Time 900 sec
1360
psi
@Temperature 180 °F,
Time 0.250 hour
Aluminum, Overlap
0.414
MPa
@Time 3600 sec
60.0
psi
@Time 1.00 hour
Aluminum, Overlap
12.5
MPa
@Time 1800 sec
1810
psi
@Time 0.500 hour
Aluminum, Overlap
18.5
MPa
@Time 14400 sec
2680
psi
@Time 4.00 hour
Aluminum, Overlap
Peel Strength
0.526
-
0.877
kN/m
@Temperature -55.0 °C
3.00
-
5.00
pli
@Temperature -67.0 °F
Aluminum, T-Peel
3.33
kN/m
@Temperature -55.0 °C
19.0
pli
@Temperature -67.0 °F
Aluminum Bell Pell; ASTM D3167
3.51
kN/m
@Temperature 82.0 °C
20.0
pli
@Temperature 180 °F
Aluminum, T-Peel
6.84
kN/m
@Temperature 82.0 °C
39.0
pli
@Temperature 180 °F
Aluminum Bell Pell; ASTM D3167
10.5
kN/m
@Temperature 23.0 °C
60.0
pli
@Temperature 73.4 °F
Aluminum, T-Peel
13.5
kN/m
@Temperature 23.0 °C
77.0
pli
@Temperature 73.4 °F
Aluminum Bell Pell; ASTM D3167
Electrical Properties
Metric
English
Comments
Volume Resistivity
3.25e+15
ohm-cm
3.25e+15
ohm-cm
ASTM D257
Dielectric Strength
28.6
kV/mm
727
kV/in
ASTM D149
Thermal Properties
Metric
English
Comments
CTE, linear
74.44
µm/m-°C
41.36
µin/in-°F
Below Tg
166
µm/m-°C
92.2
µin/in-°F
Above Tg
Thermal Conductivity
0.180
W/m-K
@Temperature 45.0 °C
1.25
BTU-in/hr-ft²-°F
@Temperature 113 °F
Descriptive Properties
Appearance
Amber
Accelerator
Off-White
White
Base
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive
3M Scotch-Weld™ 2214 Hi-Temp New Formula Epoxy Adhesive
3M Scotch-Weld™ 2214 Hi-Temp Epoxy Adhesive
PMM34648 / 169395
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.