MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotch-Weld™ 2214 Regular Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Adhesive 2214 Regular is an aluminum filled general purpose product for use in applications where high strength bonds are needed in a temperature range of -53-121°C.One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a paste consistency epoxy adhesive designed for bonding metals and many high temperature plastics such as fiberglass reinforced plastic, polyester, and phonetics

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 60 - 200 cP60 - 200 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 85>= 85
Tensile Strength, Ultimate 68.9 MPa10000 psi
Elongation at Break <= 2.0 %<= 2.0 %
Modulus of Elasticity 5.17 GPa750 ksi
Shear Strength  2.76 MPa
@Temperature 177 °C
400 psi
@Temperature 351 °F
Aluminum Overlap
 4.14 MPa
@Temperature 149 °C
600 psi
@Temperature 300 °F
Aluminum Overlap
 10.3 MPa
@Temperature 121 °C
1500 psi
@Temperature 250 °F
Aluminum Overlap
 20.7 MPa
@Temperature -53.0 °C
3000 psi
@Temperature -63.4 °F
Aluminum Overlap
 31.0 MPa
@Temperature 24.0 °C
4500 psi
@Temperature 75.2 °F
Aluminum Overlap
 31.0 MPa
@Temperature 82.0 °C
4500 psi
@Temperature 180 °F
Aluminum Overlap
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 2.80e+13 ohm-cm2.80e+13 ohm-cm
Surface Resistance 9.80e+12 ohm9.80e+12 ohm
Dielectric Constant  10.5
@Temperature 23.0 °C
10.5
@Temperature 73.4 °F
ASTM D150
 11.1
@Temperature 60.0 °C
11.1
@Temperature 140 °F
ASTM D150
 16.7
@Temperature 90.0 °C
16.7
@Temperature 194 °F
ASTM D150
 24
@Temperature 104 °C
24
@Temperature 219 °F
ASTM D150
Dielectric Strength 3.03 kV/mm
@Thickness 0.930 mm
77.0 kV/in
@Thickness 0.0366 in
Dissipation Factor  0.126
@Temperature 23.0 °C
0.126
@Temperature 73.4 °F
 0.346
@Temperature 90.0 °C
0.346
@Temperature 194 °F
 0.463
@Temperature 60.0 °C
0.463
@Temperature 140 °F
 0.515
@Temperature 104 °C
0.515
@Temperature 219 °F
Arc Resistance 76 sec76 sec
 
Thermal PropertiesMetricEnglishComments
CTE, linear 49.0 µm/m-°C
@Temperature 0.000 - 80.0 °C
27.2 µin/in-°F
@Temperature 32.0 - 176 °F
Thermal Conductivity 0.399 W/m-K2.77 BTU-in/hr-ft²-°F
 
Descriptive Properties
AppearanceGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch-Weld™ 2214 Regular Gray One-Part Epoxy Adhesive
3M Scotch-Weld™ 2214 Hi-Temp Epoxy Adhesive
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M Scotch-Weld™ 2214 Hi-Temp New Formula Epoxy Adhesive
3M Scotch-Weld™ DP460 NS Epoxy Adhesive

PMM34630 / 169377

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.