MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

3M Scotch-Weld™ 2214 Hi-Temp New Formula Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Adhesive 2214 Hi-Temp Formula is an aluminum filled, deaerated products fro use where higher strengths are required between 82-177°C. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a paste consistency epoxy adhesive designed for bonding metals and many high temperature plastics such as fiberglass reinforced plastic, polyester, and phenolics

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Viscosity 100 - 250 cP100 - 250 cP
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D >= 85>= 85
Elongation at Break 1.0 %1.0 %
Shear Strength  8.27 MPa
@Temperature 177 °C
1200 psi
@Temperature 351 °F
Aluminum Overlap
 13.8 MPa
@Temperature 149 °C
2000 psi
@Temperature 300 °F
Aluminum Overlap
 17.2 MPa
@Temperature 121 °C
2500 psi
@Temperature 250 °F
Aluminum Overlap
 19.3 MPa
@Temperature -53.0 °C
2800 psi
@Temperature -63.4 °F
Aluminum Overlap
 19.3 MPa
@Temperature 24.0 °C
2800 psi
@Temperature 75.2 °F
Aluminum Overlap
 19.3 MPa
@Temperature 82.0 °C
2800 psi
@Temperature 180 °F
Aluminum Overlap
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant  4.61
@Temperature 23.0 °C
4.61
@Temperature 73.4 °F
ASTM D150
 4.96
@Temperature 60.0 °C
4.96
@Temperature 140 °F
ASTM D150
Dissipation Factor  0.0135
@Temperature 23.0 °C
0.0135
@Temperature 73.4 °F
 0.018
@Temperature 60.0 °C
0.018
@Temperature 140 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 44.0 µm/m-°C
@Temperature -60.0 - 80.0 °C
24.4 µin/in-°F
@Temperature -76.0 - 176 °F
Thermal Conductivity 0.429 W/m-K2.98 BTU-in/hr-ft²-°F
 
Descriptive Properties
AppearanceGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive
Magnesium AZ91A-F, Die Cast
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive

PMM34633 / 169380

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.