MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
3M Scotch-Weld™ 2214 Hi-Temp New Formula Epoxy Adhesive
Categories: Polymer; Adhesive; Thermoset; Epoxy; Epoxy Adhesive

Material Notes: 3M™ Scotch-Weld™ Adhesive 2214 Hi-Temp Formula is an aluminum filled, deaerated products fro use where higher strengths are required between 82-177°C. One part 250°F (121°C) curing 100% solids, 3M™ Scotch-Weld™ Epoxy Adhesive 2214 is a paste consistency epoxy adhesive designed for bonding metals and many high temperature plastics such as fiberglass reinforced plastic, polyester, and phenolics

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 100 - 250 cP
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D >= 85
Elongation at Break 1.0 %
Shear Strength 1200 psi
@Temperature 177 °C
Aluminum Overlap
 2000 psi
@Temperature 149 °C
Aluminum Overlap
 2500 psi
@Temperature 121 °C
Aluminum Overlap
 2800 psi
@Temperature -53.0 °C
Aluminum Overlap
 2800 psi
@Temperature 24.0 °C
Aluminum Overlap
 2800 psi
@Temperature 82.0 °C
Aluminum Overlap
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 4.61
@Temperature 23.0 °C
ASTM D150
 4.96
@Temperature 60.0 °C
ASTM D150
Dissipation Factor 0.0135
@Temperature 23.0 °C
 0.018
@Temperature 60.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 44.0 µm/m-°C
@Temperature -60.0 - 80.0 °C
Thermal Conductivity 2.98 BTU-in/hr-ft²-°F
 
Descriptive Properties
AppearanceGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
3M Scotch-Weld™ DP460 Off-White Epoxy Adhesive
3M Scotch-Weld™ DP460 NS Epoxy Adhesive
3M Scotch-Weld™ 2214 Regular Epoxy Adhesive
Magnesium AZ91A-F, Die Cast
3M Scotch-Weld™ 2214 Non-Metallic Filled Epoxy Adhesive

PMM34633 / 169380

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.