MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Total PPC 5720WZ Polypropylene, Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: TOTAL Petrochemicals Polypropylene 5720WZ is a nucleated impact copolymer with a Melt Flow index of 20 g/10 min.

TOTAL Polypropylene 5720WZ is characterized by good stiffness, creep resistance, very high impact resistance, excellent antistatic properties and has been formulated to allow faster cycling through early demolding.

Total Polypropylene 5720WZ has been developed specifically for the injection molding of crates, pails, and other heavy duty articles.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.905 g/cc0.905 g/ccASTM D1505
Melt Flow 20 g/10 min20 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 23.0 MPa3340 psiASTM D638
Elongation at Yield 7.0 %7.0 %ASTM D638
Flexural Modulus 1.35 GPa196 ksiASTM D790
Izod Impact, Notched 1.80 J/cm3.37 ft-lb/inASTM D256
 
Thermal PropertiesMetricEnglishComments
Melting Point 160 - 165 °C320 - 329 °FTOTAL Method
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °C194 °FPressure unspecified; ASTM D648
Vicat Softening Point 150 °C302 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Total PPC 4280W Polypropylene, Impact Copolymer
Total PPH 3620WZ Polypropylene, Injection Molding Grade
Total PPH 3462 Polypropylene, Extrusion Grade
Total PPC 5724 Polypropylene, Extra High Impact Copolymer
Ineos N20N-00 Polypropylene Impact Copolymer

PTOTAL867 / 130592

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.