MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow DOWLEX™ 2247G Polyethylene Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE)

Material Notes: Next Generation DOWLEX™ 2247G Polyethylene Resin with Extra Stretch Performance (ESP) is an ethylene-octene-1 copolymer designated for cast stretch film applications, such as industrial pallet wrap. DOWLEX 2247G provides stretch films with superior extensibility and increased resistance to failure around film flaws while maintaining exceptional puncture resistance and load retention.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.917 g/cc0.0331 lb/in³ASTM D792
Thickness 58.4 microns2.30 mil
Melt Flow 2.3 g/10 min2.3 g/10 minASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 9.080 MPa1317 psiASTM D882
Film Tensile Strength at Yield, TD 8.846 MPa1283 psiASTM D882
Film Elongation at Break, MD 432 %432 %ASTM D882
Film Elongation at Break, TD 705 %705 %ASTM D882
Impact 321321[ft-lbf/in3]; Puncture Resistance; Dow Method
 20602060[ft-lbf/in3]; Toughness MD; ASTM D882
 26532653[ft-lbf/in3]; Toughness TD; ASTM D882
Elmendorf Tear Strength MD 295 g295 gASTM D1922
Elmendorf Tear Strength TD 558 g558 gASTM D1922
Elmendorf Tear Strength, MD 5.05 g/micron128 g/milASTM D1922
Elmendorf Tear Strength, TD 9.55 g/micron243 g/milASTM D1922
Dart Drop Test 148 g0.326 lbMethod B; ASTM D1709
Film Tensile Strength at Break, MD 50.11 MPa7268 psiASTM D882
Film Tensile Strength at Break, TD 35.9 MPa5210 psiASTM D882
 
Thermal PropertiesMetricEnglishComments
Melting Point 123 °C253 °FDow Method (DSC)
Vicat Softening Point 99.0 °C210 °FASTM D1525
 
Optical PropertiesMetricEnglishComments
Haze 0.80 %0.80 %ASTM D1003
Gloss 94.6 %94.6 %45°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow DOWLEX™ 2045G Linear Low Density Polyethylene
Dow DOWLEX™ 2037 Linear Low Density Polyethylene, Cast Film Grade
Dow DOWLEX™ 2085G Polyethylene Resin
Dow DOWLEX™ 2020G Linear Low Density Polyethylene
Dow DOWLEX™ 2021D Linear Low Density Polyethylene

PDOW1318 / 30536

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.