MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Boron, B
Categories: Metal; Nonferrous Metal; Pure Element

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 2.60 g/cc0.0939 lb/in³
a Lattice Constant 4.91 Å4.91 Å
c Lattice Constant 12.6 Å12.6 Å
 
Chemical PropertiesMetricEnglishComments
Atomic Mass 10.81110.8111995
Atomic Number 55
X-ray Absorption Edge 66.289 Å66.289 ÅK
Electronegativity 2.042.04Pauling
Ionic Radius 0.230 Å0.230 ÅCrystal Ionic Radius for Valence +3
 0.350 Å0.350 ÅCrystal Ionic Radius for Valence +1
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 33003300
Hardness, Mohs 9.59.5
Tensile Strength, Ultimate 1.60 - 2.40 MPa232 - 348 psiAmorphous
 2.60 - 3.10 MPa377 - 450 psiCrystalline
Tensile Modulus 0.440 GPa63.8 ksi
Compressive Strength <= 0.500 MPa<= 72.5 psiB2O3 inclusions
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity  0.00200 ohm-cm
@Temperature 600 °C
0.00200 ohm-cm
@Temperature 1110 °F
 0.0120 ohm-cm
@Temperature 520 °C
0.0120 ohm-cm
@Temperature 968 °F
 0.0400 ohm-cm
@Temperature 320 °C
0.0400 ohm-cm
@Temperature 608 °F
 30.0 ohm-cm
@Temperature 170 °C
30.0 ohm-cm
@Temperature 338 °F
 400 ohm-cm
@Temperature 100 °C
400 ohm-cm
@Temperature 212 °F
 6500 ohm-cm
@Temperature 25.0 °C
6500 ohm-cm
@Temperature 77.0 °F
 30000 ohm-cm
@Temperature 0.000 °C
30000 ohm-cm
@Temperature 32.0 °F
 40000 ohm-cm
@Temperature -10.0 °C
40000 ohm-cm
@Temperature 14.0 °F
 400000 ohm-cm
@Temperature -150 °C
400000 ohm-cm
@Temperature -238 °F
Magnetic Susceptibility -6.20e-7-6.20e-7cgs/g
Band Gap 1.55 eV1.55 eV
Electron Mobility, cm²/V-s 1010
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 2050 J/g882 BTU/lb
Heat of Vaporization 3140 J/g1350 BTU/lb
CTE, linear 8.20 µm/m-°C
@Temperature 20.0 - 100 °C
4.56 µin/in-°F
@Temperature 68.0 - 212 °F
Specific Heat Capacity  0.0297 J/g-°C
@Temperature -191 - -78.0 °C
0.00710 BTU/lb-°F
@Temperature -312 - -108 °F
 0.754 J/g-°C
@Temperature -76.0 - 0.000 °C
0.180 BTU/lb-°F
@Temperature -105 - 32.0 °F
 1.285 J/g-°C
@Temperature 0.000 - 100 °C
0.3071 BTU/lb-°F
@Temperature 32.0 - 212 °F
 1.62 J/g-°C
@Temperature 100 °C
0.387 BTU/lb-°F
@Temperature 212 °F
 1.976 J/g-°C
@Temperature 500 °C
0.4723 BTU/lb-°F
@Temperature 932 °F
 2.135 J/g-°C
@Temperature 900 °C
0.5103 BTU/lb-°F
@Temperature 1650 °F
Thermal Conductivity 27.4 W/m-K190 BTU-in/hr-ft²-°F
Melting Point 2300 °C4170 °F
Boiling Point 4000 °C7230 °F
Heat of Formation 397.1 kJ/mol397.1 kJ/mol
Debye Temperature 1097 °C2007 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 3.403.40
 
Component Elements PropertiesMetricEnglishComments
Boron, B 100 %100 %
 
Descriptive Properties
CAS Number7440-42-8

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Aluminum, Al
Silver, Ag
Gold, Au
Americium, Am
Chromium, Cr; Recrystallized

AMEB000 / 8

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.