MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® F522 Epoxy Resin, K285 Kevlar® Fabric  (discontinued **)
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Hexcel designation: K285-38"-F522; Kev. 49 1140

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 517 MPa
@Temperature 24.0 °C
75000 psi
@Temperature 75.2 °F
Dry
Tensile Modulus 29.0 GPa
@Temperature 24.0 °C
4210 ksi
@Temperature 75.2 °F
Dry
Flexural Yield Strength  110 MPa
@Temperature 24.0 °C
16000 psi
@Temperature 75.2 °F
Long Beam, Dry
 414 MPa
@Temperature 24.0 °C
60000 psi
@Temperature 75.2 °F
Dry
Compressive Yield Strength  117 MPa
@Temperature 71.0 °C
17000 psi
@Temperature 160 °F
Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C)
 179 MPa
@Temperature 24.0 °C
26000 psi
@Temperature 75.2 °F
Dry
Compressive Modulus  25.5 GPa
@Temperature 71.0 °C
3700 ksi
@Temperature 160 °F
Wet (14 ± 1/2 days of water immersion at 160 ± 5°F (71 ± 3°C)
 30.3 GPa
@Temperature 24.0 °C
4390 ksi
@Temperature 75.2 °F
Dry
 
Descriptive Properties
Dry Resin Content (%)49-55Prepreg
Flow (%)20-32
Wet Resin Content (%)46Laminate

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® F522 Epoxy Resin, K120 Kevlar® Fabric
Hexcel® HexPly® F185 Epoxy Resin, K285 Kevlar Fabric
Hexcel® F161 Epoxy Resin, 120 Glass Fabric
Hexcel® HexPly® F155 Epoxy Resin, K285 Kevlar Fabric
Hexcel® F161 Epoxy Resin, 285 Kevlar Fabric

PHEXC136 / 98606

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.