MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Hexcel® HexPly® F185 Epoxy Resin, K285 Kevlar Fabric
Categories: Polymer; Thermoset; Epoxy; Epoxy Cure Resin

Material Notes: Hexcel designation: 285-38"-F185; Fiber: Kev. 49 1140

Information provided by HexCel

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Filler Content 42.0 %42.0 %Laminate Fiber Volume
Volatiles 0.40 - 1.2 %0.40 - 1.2 %Prepreg
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield  419 MPa
@Temperature 24.0 °C
60800 psi
@Temperature 75.2 °F
Fill TS
 507 MPa
@Temperature 24.0 °C
73500 psi
@Temperature 75.2 °F
Warp TS
Tensile Modulus  24.0 GPa
@Temperature 24.0 °C
3480 ksi
@Temperature 75.2 °F
Warp tensile modulus
 26.3 GPa
@Temperature 24.0 °C
3810 ksi
@Temperature 75.2 °F
Fill tensile modulus
Compressive Yield Strength  155 MPa
@Temperature 24.0 °C
22500 psi
@Temperature 75.2 °F
Warp compression
 164 MPa
@Temperature 24.0 °C
23800 psi
@Temperature 75.2 °F
Fill compression
Compressive Modulus  13.8 GPa
@Temperature 24.0 °C
2000 ksi
@Temperature 75.2 °F
Fill compression
 19.3 GPa
@Temperature 24.0 °C
2800 ksi
@Temperature 75.2 °F
Warp compression
Shear Strength 36.0 MPa
@Temperature 24.0 °C
5220 psi
@Temperature 75.2 °F
Warp short beam shear
 
Descriptive Properties
Cured Thickness per Ply (cm)0.028Laminate
Flow (%)24-34
Wet Resin Content (%)52-58Prepreg

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Hexcel® HexPly® F155 Epoxy Resin, K120 Kevlar Fabric
Hexcel® HexPly® F522 Epoxy Resin, K285 Kevlar® Fabric
Arlon Electronic Materials 45NK Woven Kevlar® Reinforced Laminate and Prepreg
Hexcel® F161 Epoxy Resin, 285 Kevlar Fabric
Hexcel® F161 Epoxy Resin, 120 Glass Fabric

PHEXC117 / 98587

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.