MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Dow SiLK™ I300 560 Semiconductor Dielectric Resin  (discontinued **)
Categories: Polymer

Material Notes: SiLK™ I300 560 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I300 560 is compatible with standard IC processing tools in todays fabrications. SiLK™ I300 560 is fluorine-free, thus is compatible with Ti and Ta barrier materials.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Moisture Absorption 0.24 %0.24 %80% R.H.
Thickness 0.560 microns0.0220 mil3000 rpm
 0.485 - 0.685 microns0.0191 - 0.0270 mil2000-4000 rpm
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 89.0 MPa12900 psi
Tensile Strength, Yield 60.0 MPa8700 psi
Tensile Modulus 2.45 GPa355 ksi
 
Electrical PropertiesMetricEnglishComments
Dielectric Constant 2.6
@Frequency 100000 Hz
2.6
@Frequency 100000 Hz
Dielectric Strength >= 400 kV/mm>= 10200 kV/in
 
Thermal PropertiesMetricEnglishComments
CTE, linear 62.0 µm/m-°C
@Temperature 50.0 - 150 °C
34.4 µin/in-°F
@Temperature 122 - 302 °F
Thermal Conductivity 0.190 W/m-K1.32 BTU-in/hr-ft²-°F
 0.230 W/m-K
@Temperature 125 °C
1.60 BTU-in/hr-ft²-°F
@Temperature 257 °F
Glass Transition Temp, Tg >= 490 °C>= 914 °F
Decomposition Temperature 450 °C842 °F1% weight loss per hour
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.631.63

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Dow C133-02 Polypropylene Impact Copolymer Resin
SK Chemicals Saran® 506 Polymer
Dow Tyrin® CM0730 Chlorinated Polyethylene Elastomer
Dow SPECTRIM™ 50-S Reaction Moldable Polymer
Dow INSPIRE™ 112 Performance Polymer

PDOW1073 / 30277

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.