MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Sandvik H6N 6% Cobalt Binder Cemented Carbide, Seal Grade  (discontinued **)
Categories: Ceramic; Carbide; Metal; Metal Matrix Composite; Nonferrous Metal; Tungsten Alloy

Material Notes: Sandvik seal grade H6N is a standard/straight cobalt binder grade. This grade shows excellent wear resistance combined with high toughness. Due to the cobalt binder, this grade is not recommended for applications in corrosive environments.

Features:

  • 6% cobalt binder, 94% tungsten carbide. The carbide grain size is medium.
  • Very good wear resistance
  • High toughness
  • Relatively low to medium corrosion resistance –particularly to aqueous solutions, due to the cobalt binder.
  • Good brazeability
  • Information provided by Sandvik

    Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
     
    Physical PropertiesMetricEnglishComments
    Density 14.95 g/cc0.5401 lb/in³
     
    Mechanical PropertiesMetricEnglishComments
    Hardness, Rockwell A 91.991.9
    Hardness, Vickers 1575157530
    Flexural Strength 2200 MPa319000 psiTransverse Rupture; ISO 3327
    Compressive Strength 6200 MPa899000 psi
     
    Component Elements PropertiesMetricEnglishComments
    Cobalt, Co 6.0 %6.0 %
    WC 94 %94 %
     
    Descriptive Properties
    Corrosion Resistance, 1-104
    Wear Resistance, 0-108

    **
    Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

    Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

    Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

    Users viewing this material also viewed the following:
    Sandvik PN90 Nano-Series Cemented Carbide for Metal Forming Applications
    Sandvik C6N 6% Nickel Binder Cemented Carbide, Seal Grade
    Sandvik H11N Cemented Carbide for Metal Forming Applications
    Sapco Si.SiC Silicon Carbide
    Tungsten Carbide, WC

    NSANDV009 / 18903

    Free Trade Publications, Click Here!
    Free Trade Publications, Click Here!

    Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

    The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.