MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Braskem Idealis 500 High Molecular Weight Polyethylene Powder  (discontinued **)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: Braskem Idealis 500 is the only High Molecular Weight Polyethylene resin in powder form specially designed for the compression molding process; Applications range from food handling cutting boards and playground toys to technical parts.

Information provided by Braskem.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.951 g/cc0.951 g/ccASTM D792
Bulk Density 0.450 g/cc0.0163 lb/in³ASTM D1895
Particle Size 195 µm195 µmAverage; Dp50; ASTM D1921
Viscosity Test 470 cm³/g4.70 dl/gIntrinsic; ASTM D4020
Molecular Weight 550000 g/mol550000 g/molBraskem
Melt Flow 0.70 g/10 min
@Load 21.6 kg,
Temperature 190 °C
0.70 g/10 min
@Load 47.6 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 63
@Time 15.0 sec
63
@Time 0.00417 hour
ASTM D2240
Tensile Strength at Break >= 30.0 MPa>= 4350 psiASTM D638
Tensile Strength, Yield >= 20.0 MPa>= 2900 psiASTM D638
Elongation at Break >= 500 %>= 500 %ASTM D638
Flexural Modulus 0.930 GPa135 ksiASTM D790
Charpy Impact, Notched >= 5.00 J/cm²>= 23.8 ft-lb/in²Determined with double-notched specimens; ISO 11542-2
Abrasion 8080Braskem (PE500 = 100)
 
Thermal PropertiesMetricEnglishComments
Melting Point 136 °C277 °FASTM D3418
Vicat Softening Point 80.0 °C
@Load 5.10 kg
176 °F
@Load 11.2 lb
ASTM D1525

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Braskem UTEC® 3040 Ultra High Molecular Weight Polyethylene
Braskem UTEC® 4040 Ultra High Molecular Weight Polyethylene
Polikim ULPOLEN® 1000 UHMWPE Standard
Braskem UTEC® 5041 Ultra High Molecular Weight Polyethylene
Braskem UTEC® 5040 Ultra High Molecular Weight Polyethylene

PBRAS750 / 109477

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.