MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

BASF Ultramid® A3X2G7 BK 23187 35% Glass Filled PA66 FR (Dry)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Description: 35% glass-fiber reinforced injection-molding grade with improved flame retardance and enhanced long-term stability. Flame retardant based on red phosphorus; very high stiffness and strength; outstanding mechanical and electrical properties.

Information provided by BASF

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.500 - 0.800 g/cc0.0181 - 0.0289 lb/in³
Density 1.45 g/cc0.0524 lb/in³ISO 1183
Moisture Absorption at Equilibrium 1.0 - 1.4 %1.0 - 1.4 %23°C; 50% RH; ISO 62
Water Absorption at Saturation 4.4 - 5.0 %4.4 - 5.0 %ISO 62
Viscosity Measurement 140140ISO 307
Linear Mold Shrinkage 0.0045 cm/cm0.0045 in/inrestricted
Linear Mold Shrinkage, Flow 0.0034 cm/cm0.0034 in/inISO 2577
Linear Mold Shrinkage, Transverse 0.0114 cm/cm0.0114 in/inISO 2577
Melt Flow 43.5 g/10 min
@Load 5.00 kg,
Temperature 275 °C
43.5 g/10 min
@Load 11.0 lb,
Temperature 527 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Yield 160 MPa23200 psi50 mm/min; ISO 527-1/-2
Elongation at Yield 3.0 %3.0 %50 mm/min; ISO 527-1/-2
Modulus of Elasticity 11.0 GPa1600 ksiISO 527-1/-2
Flexural Modulus 9.20 GPa1330 ksiISO 178
Izod Impact, Notched (ISO) 13.0 kJ/m²
@Temperature 23.0 °C
6.19 ft-lb/in²
@Temperature 73.4 °F
ISO 180/A
Charpy Impact Unnotched  6.50 J/cm²
@Temperature -30.0 °C
30.9 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eU
 7.00 J/cm²
@Temperature 23.0 °C
33.3 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eU
Charpy Impact, Notched  1.00 J/cm²
@Temperature -30.0 °C
4.76 ft-lb/in²
@Temperature -22.0 °F
ISO 179/1eA
 1.40 J/cm²
@Temperature 23.0 °C
6.66 ft-lb/in²
@Temperature 73.4 °F
ISO 179/1eA
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+13 ohm-cm1.00e+13 ohm-cmIEC 60093
Dielectric Constant 3.6
@Frequency 1e+6 Hz
3.6
@Frequency 1e+6 Hz
IEC 60250
Dissipation Factor 0.020
@Frequency 1e+6 Hz
0.020
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 V600 VTest solution A; IEC 60112
Hot Wire Ignition, HWI 2.0 sec
@Thickness >=0.750 mm
2.0 sec
@Thickness >=0.0295 in
ASTM D3874-88
High Amp Arc Ignition, HAI 0.00 arcs
@Thickness >=0.400 mm
0.00 arcs
@Thickness >=0.0157 in
UL 746C
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.0 - 20.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
8.33 - 11.1 µin/in-°F
@Temperature 73.4 - 176 °F
DIN 11359-1/-2
CTE, linear, Transverse to Flow 60.0 - 70.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
33.3 - 38.9 µin/in-°F
@Temperature 73.4 - 176 °F
DIN 11359-1/-2
Specific Heat Capacity 1.40 J/g-°C0.335 BTU/lb-°F
Thermal Conductivity 0.340 W/m-K2.36 BTU-in/hr-ft²-°FDIN 52612
Melting Point 260 °C500 °FDIN 53765
Maximum Service Temperature, Air 140 °C284 °Ffor 50% loss of tensile strength after 20000hr
 157 °C315 °Ffor 50% loss of tensile strength after 5000hr
 220 °C428 °F
Deflection Temperature at 0.46 MPa (66 psi) 250 °C482 °FISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 250 °C482 °FISO 75-1/-2
Decomposition Temperature >= 310 °C>= 590 °F
UL RTI, Electrical 115 °C
@Thickness 1.50 mm
239 °F
@Thickness 0.0591 in
UL 746B
Flammability, UL94  HB
@Thickness >=0.400 mm
HB
@Thickness >=0.0157 in
 V-0
@Thickness >=0.750 mm
V-0
@Thickness >=0.0295 in
 5VB
@Thickness >=1.50 mm
5VB
@Thickness >=0.0591 in
Oxygen Index 28 %28 %ISO 4589-2
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
1760 °F
@Thickness 0.0315 in
IEC 60695-2-12
Ignition Temperature >= 350 °C>= 662 °FASTM D1929
 
Processing PropertiesMetricEnglishComments
Processing Temperature 80.0 °C176 °FHopper Throat
Zone 1 290 °C554 °FFeed Zone
Zone 2 290 °C554 °FCompression
Zone 3 290 °C554 °FMetering-zone
Zone 4 290 °C554 °FNozzle
Melt Temperature 280 - 300 °C536 - 572 °FInjection-molding/Extrusion
 290 °C554 °FOptimal
Mold Temperature 80.0 °C176 °FOptimal
 80.0 - 90.0 °C176 - 194 °FInjection-molding
Drying Temperature 80.0 °C176 °F
Dry Time 4 hour4 hour
Moisture Content 0.030 - 0.060 %0.030 - 0.060 %Optimal
 <= 0.15 %<= 0.15 %
 
Descriptive Properties
ColorBK 23187
Commercial StatusEurope
Peripheral Screw Speed< 0.3 m/s

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
BASF Ultramid® A3X2G7 BK 23187 35% Glass Filled PA66 FR (Conditioned)
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Conditioned)
BASF Ultramid® A3X2G7 35% Glass Filled PA66 (Dry)
BASF Ultramid® A3X2G5 25% Glass Filled PA66 (Dry)
BASF Ultramid® FRee A3U40G5 25% Glass Filled PA66 FR (Dry)

PBASG0312 / 131945

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.