MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Trinseo CALIBRE™ 201-10 Polycarbonate Resin
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: CALIBRE™ 200-10 is produced in compliance with the US FDA and EU food contact regulations. It provides excellent impact resistance, heat distortion resistance and optical clarity. CALIBRE 200-10 product is formulated with mold release.

Applications:

  • Food processor housings
  • Liquid containers
  • Food utensils
  • Packaging applications
Govt. and Industry Standards:
  • US FDA 21 CFR 177.1580
  • Underwriters Laboratory (UL)
  • EU food contact 2002/72/EC

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.20 g/cc0.0434 lb/in³ISO 1183/A
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm0.0050 - 0.0070 in/inISO 294-4
Melt Flow 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
10 g/10 min
@Load 2.65 lb,
Temperature 572 °F
ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 71.0 MPa10300 psiISO 527-2/50
Tensile Strength, Yield 60.0 MPa8700 psiISO 527-2/50
Elongation at Break 150 %150 %ISO 527-2/50
Elongation at Yield 6.0 %6.0 %ISO 527-2/50
Tensile Modulus 2.30 GPa334 ksiISO 527-2/50
Flexural Strength 97.0 MPa14100 psi2.0 mm/min; ISO 178
Flexural Modulus 2.40 GPa348 ksi2.0 mm/min; ISO 178
Izod Impact, Notched (ISO) 88.0 kJ/m²41.9 ft-lb/in²ISO 180/A
Izod Impact, Unnotched (ISO) NBNBISO 180
 
Electrical PropertiesMetricEnglishComments
Comparative Tracking Index 250 V
@Thickness 2.00 mm
250 V
@Thickness 0.0787 in
Solution A; IEC 60112
 
Thermal PropertiesMetricEnglishComments
Hot Ball Pressure Test 125 °C257 °FIEC 60335-1
Deflection Temperature at 0.46 MPa (66 psi) 144 °C291 °FAnnealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 125 °C257 °FUnannealed; ISO 75-2/A
 141 °C286 °FAnnealed; ISO 75-2/A
Vicat Softening Point 149 °C300 °FISO 306/B50
Flammability, UL94  HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
 HB
@Thickness 3.20 mm
HB
@Thickness 0.126 in
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 87 - 91 %87 - 91 %ASTM D1003
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LG Chemical Lupoy 1201-10 Polycarbonate Resin
RTP Company RTP 300 HF FR A Polycarbonate (PC), High Flow - Unreinforced - Flame Retardant - UL94 V-0
Trinseo CALIBRE™ 200-10 Polycarbonate Resin
Trinseo CALIBRE™ 201-22 Polycarbonate Resin
Trinseo CALIBRE™ 201-6 Polycarbonate Resin

PDWST010 / 142219

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.