MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Trinseo TYRIL™ 875 SAN Resin
Categories: Polymer; Thermoplastic; SAN Polymer

Material Notes: TYRIL™ styrene-acrylonitrile (SAN) resins are designed to offer superior chemical resistance, strength, hardness and dimensional stability in a broad range of product applications. The key property of TYRIL 875 is specifically designed to provide good processability, good chemical resistance, heat resistance, very good strength and optimal aesthetics.

Applications:

  • Small appliances: transparent kitchen-robot parts

Information provided by Trinseo.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.08 g/ccISO 1183
Apparent Bulk Density 0.690 g/ccISO 60
Melt Flow 6.5 g/10 min
@Load 3.80 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 MPaISO 527-2/5
Tensile Modulus 3700 MPaISO 527-2/5
Flexural Strength 97.0 MPa3 point load, 2.0 mm/min; ASTM D790
Charpy Impact Unnotched 17.0 kJ/m²ISO 179/1eU
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 101 °CAnnealed; ISO 75-2/A
Vicat Softening Point 111 °CISO 306/A120
Flammability, UL94 HB
@Thickness 1.50 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Trinseo CALIBRE™ 2061-15 Polycarbonate Resin
Dow Tyril® 100 SAN
Trinseo CALIBRE™ 2061-22 Polycarbonate Resin
Arkema OREVAC® 18910 Maleic Anhydride Modified Copolymer
Envalior Pocan® AF 4130 000000 PBT, 30% Glass Fiber Reinforced

PDWST091 / 142300

Elmet Technologies

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.