MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPC 4624WZ Polypropylene, Impact Copolymer
Categories: Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: ATOFINA 4624WZ polypropylene is a nucleated impact copolymer, combining good fluidity and mechanical properties. 4624WZ is characterized by significantly improved resistance, while maintaining excellent antistatic properties and good processability.

Application

ATOFINA 4624WZ has been developed specifically for the injection molding of buckets, pails, toys, housewares and garden furniture.

Information provided provided by Total Petrochemicals.

Total Petrochemicals acquired former Fina and Atofina plastics product lines.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.905 g/ccASTM D1505
Melt Flow 13 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 3770 psiASTM D638
Elongation at Yield 7.0 %ASTM D638
Flexural Modulus 167000 psiASTM D 790
Izod Impact, Notched 200 J/mASTM D256
 65.0 J/m
@Temperature -20.0 °C
ASTM D256
Charpy Impact Unnotched 1.90 J/cm²Notched/Unnotched not specified; ASTM DIN53453
 0.700 J/cm²
@Temperature -20.0 °C
Notched/Unnotched not specified; ASTM DIN53453
 
Thermal PropertiesOriginal ValueComments
Melting Point 160 - 165 °CATOFINA Method
Deflection Temperature at 0.46 MPa (66 psi) 90.0 °CASTM D648
Vicat Softening Point 148 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ExxonMobil PP7032E2 Impact Copolymer
Total PPC 4524WZ Polypropylene, Impact Copolymer
Total PPC 4280W Polypropylene, Impact Copolymer
Total PPC 4252 Polypropylene, Impact Copolymer Corrugated Sheet
ExxonMobil Santoprene® 211-87 Thermoplastic Elastomer

PFINAA071 / 38507

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.