MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CoorsTek ZDY Yttria Fully Stabilized Zirconia
Categories: Ceramic; Oxide; Zirconium Oxide

Material Notes: Oxygen ionic conductor for high-stress and high-thermal-shock environments

Key Words: ZrO2
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 5.60 g/ccASTM-C 20
Water Absorption 0.00 %ASTM-373
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell 45 N 75
Modulus of Elasticity 173 GPaASTM-C848
Flexural Strength 207 MPaMOR; ASTM-F417
Fracture Toughness 3.00 MPa-m½Notched Beam
 
Thermal PropertiesOriginal ValueComments
CTE, linear 10.5 µm/m-°C
@Temperature 25.0 - 1000 °C
ASTM-C372
Thermal Conductivity 2.20 W/m-KASTM-C408
Maximum Service Temperature, Air 2400 °CNO-LOAD COND.
 
Descriptive Properties
ColorIvory
PermeabilityGas tight
Thermal Shock Resistance (°C)200 ΔTc

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
CoorsTek Yttria Partially Stabilized Zirconia, YTZP, Sintered
Aluminum Nitride, AlN
Alumina, alpha Al2O3, 99.5%
CoorsTek PlasmaPure™ AD-998 Alumina (nom. 99.8% Al2O3)
CoorsTek PlasmaPure-UC™ 99.9% Alumina

CCOOR921 / 104625

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.