MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Polimeros Mexicanos Rotolene® Industrial Black Linear Medium Density Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Medium Density (MDPE); Linear Medium Density Polyethylene (LMDPE), Rotational Molded

Material Notes: Hexene Copolymer Linear Medium Density Polyethylene grade which is fully UV8 stabilized. High quality Polyethylene compounded in black, formulated for rotational molding applications requiring excellent mechanical and environmental resistance properties. Available as black powder.

Applications: High quality Polyethylene recommended for producing industrial tanks, cisterns, agricultural tanks, chemical tanks or for applications requiring excellent chemical resistance, impact strength and ESCR resistance. Molded parts have a smooth surface finish. This product contains mold release internal agents which eliminate the application of mold release products in the mold inner surface.

The carrier of this product meets all FDA requirements as specified in 21 CFR 177.1520 and CONEG (as a compound), covering safe use in articles for direct food contact.

Information provided by Polimeros Mexicanos

Key Words: Recommended for industrial tanks, cisterns, agricultural tanks, chemical tanks, etc.
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.938 g/ccASTM D1505
ESCR 100% Igepal® >= 900 hourASTM D1693
ESCR 10% Igepal® >= 900 hourASTM D1693
Melt Flow 3.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 2900 psi2 in/min; ASTM D638
Tensile Strength, Yield 2700 psi2 in/min; ASTM D638
Elongation at Break >= 900 %ASTM D638
Elongation at Yield 11 %ASTM D638
Flexural Modulus, 1% Secant 110000 psiASTM D790
Impact Test 50.0 ft-lb
@Temperature -40.0 °C
0.125 in.; ARM STD test
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 60.0 °CASTM D648
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
ProcessRotational Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Polimeros Mexicanos Rotolene® 93835-TG Medium Density Polyethylene
Polimeros Mexicanos Rotolene® ECO-BLACK Linear Medium Density Polyethylene
Polimeros Mexicanos Rotolene® Natural Linear Medium Density Polyethylene
Polimeros Mexicanos Rotolene® 93050 Medium Density Polyethylene
Polimeros Mexicanos Rotolene® Black Plus Polyethylene

PMEXIC992 / 157468

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.