MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Ethydco Advancene™ bEE-4909-AAH High Density Polyethylene Resin
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: Blown film. A bimodal high molecular weight high density ethylene-hexene copolymer produced using Advanced Gas phase PE Process in a single reactor. Its high molecular weight, bimodal molecular weight distribution and optimum density results in films with high strength, high rigidity and excellent processability. Tubular films of ADVANCENE™ bEE-4906AAH resin are recommended for high toughness and drawdown makes this resin ideal for downgauging in many applications. Films are readily treated and printed to give high quality graphics. It is compatible with color concentrates thus permitting the production of a variety of colored films that serve as protective and attractive decorative wraps. Main Characteristics: hexene high density resin, bimodal molecular weight distribution, high film strength, excellent processability and drawdown.

Extrusion Notes: 50mm screw size, 21:1 ration L/D, grooved screw type, 1.5mm die gap, 14 kgs/hr/mm of die circumference output, 120 mm die diameter, 4 to 1 blow up ratio, 97 rpm screw speed, 960 mm frost line height.

Information provided by ETHYDCO.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.949 g/ccASTM D792
Thickness 12.7 microns
High Load Melt Index 9.0 g/10 min
@Load 21.6 kg,
Temperature 190 °C
ASTM D1238, ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 32.0 MPa
@Thickness 0.0127 mm
ASTM D882
Film Tensile Strength at Yield, TD 30.0 MPa
@Thickness 0.0127 mm
ASTM D882
Film Elongation at Break, MD 350 %
@Thickness 0.0127 mm
ASTM D882
Film Elongation at Break, TD 350 %
@Thickness 0.0127 mm
ASTM D882
Puncture Energy 0.940 Junivation method
Elmendorf Tear Strength MD 11 g
@Thickness 0.0127 mm
method B; ASTM 1922, ISO 6383-2
Elmendorf Tear Strength TD 24 g
@Thickness 0.0127 mm
method B; ASTM 1922, ISO 6383-2
Dart Drop Test 260 g
@Thickness 0.0127 mm
ASTM 1709A, ISO 7765
Film Tensile Strength at Break, MD 71.0 MPa
@Thickness 0.0127 mm
ASTM D882
Film Tensile Strength at Break, TD 68.0 MPa
@Thickness 0.0127 mm
ASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 130 °Cunivation method (ASTM D3418, ISO 3146)
 200 - 215 °Cextrusion

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Ethydco Advancene™ EE-4811-AAH High Density Polyethylene Resin
Ethydco Advancene™ EE-4010-AAH HDPE Pipe Extrusion
Ethydco Advancene™ bEE-4906-AAH HDPE Pipe Extrusion
Ethydco Advancene™ EM-5204-UVH High Density Polyethylene Resin
Ethydco Advancene™ EE-3914-AAH Medium Density Polyethylene Resin

PETHYD905 / 200051

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.