MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Covestro Makrolon® RW 2407 Polycarbonate
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: low viscosity; easy release; UV stabilized; variable content of filler for high reflectance application; injection molding

Mechanical property data for samples at 50% RH.

Information provided by Covestro.

Key Words: RW2407
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.24 - 1.34 g/cc0.0448 - 0.0484 lb/in³ISO 1183-1
Melt Flow 19 g/10 min
@Load 1.20 kg,
Temperature 300 °C
19 g/10 min
@Load 2.65 lb,
Temperature 572 °F
cm3/10 min volume rate; ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength at Break 50.0 - 60.0 MPa
@Temperature 23.0 °C
7250 - 8700 psi
@Temperature 73.4 °F
5mm/min; ISO 527-1,-2
Tensile Strength, Yield 60.0 MPa8700 psi5mm/min; ISO 527-1,-2
Elongation at Break >= 50 %>= 50 %5mm/min; ISO 527-1,-2
 80 - 110 %80 - 110 %5mm/min; ISO 527-1,-2
Elongation at Yield 5.5 %5.5 %5mm/min; ISO 527-1,-2
Tensile Modulus 2.50 - 2.70 GPa363 - 392 ksi1mm/min; ISO 527-1,-2
Flexural Strength 96.0 MPa13900 psi2mm/min; ISO 178
 75.0 - 80.0 MPa
@Strain 3.5 %
10900 - 11600 psi
@Strain 3.5 %
2mm/min; ISO 178
Flexural Modulus 2.50 - 2.75 GPa363 - 399 ksi2mm/min; ISO 178
Flexural Strain at Break 6.0 - 6.5 %6.0 - 6.5 %2 mm/min; ISO 178
Izod Impact, Notched (ISO) 15.0 kJ/m²
@Temperature 23.0 °C
7.14 ft-lb/in²
@Temperature 73.4 °F
complete break; ISO 7391/b.o. ISO 180-A
Charpy Impact Unnotched NB
@Temperature 23.0 °C
NB
@Temperature 73.4 °F
50%RH, complete break; ISO 179 1eU
Puncture Energy 43.0 - 50.0 J31.7 - 36.9 ft-lbISO 6603-2
 
Thermal PropertiesMetricEnglishComments
Vicat Softening Point 144 °C291 °F50N, 50°C/h; ISO 306
UL RTI, Electrical 125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
UL 746B
UL RTI, Mechanical with Impact 115 °C
@Thickness 1.50 mm
239 °F
@Thickness 0.0591 in
UL 746B
UL RTI, Mechanical without Impact 125 °C
@Thickness 1.50 mm
257 °F
@Thickness 0.0591 in
UL 746B
Flammability, UL94 V-2V-2WT
 HB
@Thickness 3.00 mm
HB
@Thickness 0.118 in
WT
 HB
@Thickness 2.70 mm
HB
@Thickness 0.106 in
WT
 V-2
@Thickness 0.750 mm
V-2
@Thickness 0.0295 in
WT
Glow Wire Flammability Index  850 °C
@Thickness 0.750 mm
1560 °F
@Thickness 0.0295 in
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
1760 °F
@Thickness 0.118 in
IEC 60695-2-12
 
Optical PropertiesMetricEnglishComments
Transmission, Visible 96 - 97 %
@Thickness 4.00 mm
96 - 97 %
@Thickness 0.157 in
JIS 8722
 
Processing PropertiesMetricEnglishComments
Melt Temperature 280 °C536 °Finjection molding; ISO 294
Mold Temperature 80.0 °C176 °Finjection molding; ISO 294
 
Descriptive Properties
Puncture Maximum Force (N)4800-5100 N, ISO 6603-2

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Covestro Makrolon® 2407 Polycarbonate, Injection Grade
Covestro Makrolon® Rx1805 Polycarbonate
Covestro Makrolon® RW 2405 Polycarbonate, 10% Glass Fiber
Covestro Bayblend® FR 110 Polycarbonate/ABS Blend
Covestro Makrolon® EM 9417 Polycarbonate, 10% Glass Fiber

PB095102 / 200143

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.