MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Total PPC 4170 Polypropylene, Impact Copolymer, Blown Film Grade
Categories: Polymer; Film; Thermoplastic; Polypropylene (PP); Polypropylene, Film Grade

Material Notes: TOTAL Petrochemicals Polypropylene 4170 is a polypropylene impact copolymer grade with good melt strength for use in the extrusion of blown films.

Benefits. 4170 forms tough films with high dart impact strength, high heat resistance and excellent processability.

FDA. 4170 complies with FDA regulations in paragraph (c) 3.2a of 21 CFR Section 177.1520 and may be used for articles or components of articles for contacting food during cooking.

Recommended Applications. 4170 is recommended for use in blown film processes for the manufacture of heavy-duty bags, higher temperature requirement films, and matte finish labels. It can be used pure or in a variety of blended formulations for monolayer of co-extrusion applications.

Information provided by Total Petrochemicals.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.905 g/ccASTM D1505
Water Vapor Transmission 0.450 g/100 in²/day
@Temperature 37.8 °C
100% RH; ASTM F1249
Oxygen Transmission Rate 135 cc/100 in²/day
@Temperature 22.8 °C
0% RH; ASTM D3985
Melt Flow 0.75 g/10 min
@Temperature 230 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Tensile Strength at Yield, MD 3800 psiASTM D882
Film Tensile Strength at Yield, TD 3600 psiASTM D882
Film Elongation at Break, MD 750 %ASTM D882
Film Elongation at Break, TD 770 %ASTM D882
2% Secant Modulus 87000 psiTD; ASTM D882
 100000 psiMD; ASTM D882
Elmendorf Tear Strength MD 55 gASTM D1922
Elmendorf Tear Strength TD 300 gASTM D1922
Dart Drop Test 350 gASTM D1709, Method A
Film Tensile Strength at Break, MD 8500 psiASTM D882
Film Tensile Strength at Break, TD 5500 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 320 - 329 °FDSC
 
Optical PropertiesOriginal ValueComments
Haze 72 %ASTM D1003
Gloss 7.0 %at 45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 210 - 250 °C
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Total PPR 3221 Random Copolymer Polypropylene, Blow Molding and Sheet Extrusion
Total PPC 4252 Polypropylene, Impact Copolymer Corrugated Sheet
Total PPC 5660 Propylene, Heterophasic Copolymer
Total PPC 4280W Polypropylene, Impact Copolymer
Chevron Phillips Marlex® D139 m-LLDPE Linear Low Density Polyethylene

PTOTAL862 / 130587

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.