MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
PolyMirae Clyrell RC5056 Injection Molding Grade Polypropylene
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene, Molded

Material Notes: Clyrell RC5056 is a Random copolymer with Super High Clarity, high gloss, excellent transparency, combined with its balance of rigidity and impact, this grade is selected by customers for use in injection molding applications. Clyrell RC5056 complies with FDA cooking condition.

Product Features: Clyrell RC5056 is a Random copolymer with Super High Clarity, high gloss, excellent transparency, combined with its balance of rigidity and impact, this grade is selected by customers for use in injection molding applications. Clyrell RC5056 complies with FDA cooking condition.

Typical Applications: Baby Bottle/Transparency container/Houseware/Injection Molding/Food container/ISBM

Information provided by PolyMirae

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Melt Flow 10 g/10 min
@Load 2.16 kg,
Temperature 230 °C
Condition L; ASMT D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 102ASTM D785
Tensile Strength, Yield 350 kg(f)/cm²ASTM D638
Elongation at Yield 10 %ASTM D638
Flexural Modulus 14000 kg(f)/cm²ASTM D790
Izod Impact, Notched 5.00 kg-cm/cm
@Temperature 23.0 °C
ASTM D256
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 100 °CASTM D648
Vicat Softening Point 134 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 9.0 %
@Thickness 2.00 mm
ASTM D1003
 
Compliance PropertiesOriginal ValueComments
FDA Yes

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis HF955MO Polypropylene Homopolymer for Injection Molding
LyondellBasell Moplen HP500N Polypropylene
Ineos B4020N1331 Polyethylene Copolymer
Wacker Elastosil® LR 3043/40 A/B Liquid Silicone Rubber
PolyMirae Moplen EP500N Injection Molding Grade Polypropylene

PMIRAF50 / 183271

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.